MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials PEARLTHANE® 11T98 Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: PEARLTHANE® 11T98 is a polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, combining high hardness with excellent mechanical properties. It can be extruded and injection-molded. PEARLTHANE® 11T98 when extruded, is used for making tubing, profiles and a variety of technical parts. When processed by injection molding, can be used for making sport shoe soles (football, golf shoes), wheels, seals, etc.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9898ISO 868
Hardness, Shore D 5252ISO 868
Tensile Strength, Yield 40.1 MPa5810 psiISO 527-2/5A/500
Elongation at Break 470 %470 %ISO 527-2/5A/500
100% Modulus 16.03 MPa
@Strain 100 %
2325 psi
@Strain 100 %
ISO 527-2/5A/500
300% Modulus 29.06 MPa
@Strain 300 %
4215 psi
@Strain 300 %
ISO 527-2/5A/500
Tear Strength 175 kN/m1000 plinicked; ISO 34-1B
Abrasion 2525Resistance (mm³); ISO 4649-A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 116 °C241 °FISO 306 (A50)
 
Processing PropertiesMetricEnglishComments
Zone 1 200 °C392 °F
Zone 2 210 °C410 °F
Zone 3 215 °C419 °F
Zone 4 220 °C428 °F
Adapter Temperature 220 °C428 °F(5)
Die Temperature 220 °C428 °FTIP (7)
 220 °C428 °F(6)
Dry Time 100 hour
@Time 10800 - 14400 sec
100 hour
@Time 3.00 - 4.00 hour
 
Descriptive Properties
Compression Zone205°C
Metering Zone215°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Total PPC 9712 Polypropylene, Heterophasic Copolymer
Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer

PMES34 / 88411

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.