MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M 7247 Thermal Transfer Polyester with TT3 Matte Topcoating Label Material
Categories: Polymer; Adhesive

Material Notes: 3M™ Thermal Transfer Polyester Label Materials offer supreme image durability in harsh environments. The polyester label stock utilizes 3M™ Adhesive 350, which is designed to permanently bond to high and low surface energy plastics, textured and contoured surfaces, powder coatings and slightly oily metals

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 1.80 milAdhesive
 2.20 milFacestock
 2.20 milLiner
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 2.25 pliHDPE, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 2.3125 pliHDPE, 90° Peel, Initial 20 min dwell at RT; FTM 2
 2.875 pliLDPE, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 2.875 pliHDPE, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 3.0625 pliPolypropylene, 90° Peel, Initial 20 min dwell at RT; FTM 2
 3.0625 pliLDPE, 90° Peel, Initial 20 min dwell at RT; FTM 2
 3.25 pliLDPE, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 3.5625 pliAluminum, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 3.5625 pliPowder Coating, 90° Peel, Initial 20 min dwell at RT; FTM 2
 3.625 pliPolypropylene, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 3.8125 pliPhenolic, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 3.8125 pliPhenolic, 90° Peel, Initial 20 min dwell at RT; FTM 2
 3.875 pliAluminum, 90° Peel, Initial 20 min dwell at RT; FTM 2
 3.875 pliABS, 90° Peel, Initial 20 min dwell at RT; FTM 2
 3.875 pliPolystyrene, 90° Peel, Initial 20 min dwell at RT; FTM 2
 4.00 pliPolycarbonate, 90° Peel, Initial 20 min dwell at RT; FTM 2
 4.125 pliPolypropylene, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 4.1875 pliPolycarbonate, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 4.1875 pliStainless Steel, 90° Peel, Initial 20 min dwell at RT; FTM 2
 4.25 pliPolystyrene, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 4.25 pliPolystyrene, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 4.25 pliABS, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 4.3125 pliPowder Coating, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 4.50 pliStainless Steel, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 4.625 pliPolycarbonate, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 4.8125 pliPhenolic, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 5.00 pliABS, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 5.1875 pliPowder Coating, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 5.3125 pliAluminum, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 6.1875 pliStainless Steel, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Adhesive Type350 Acrylic
Liner40# White Densified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M 7222/7865 Thermal Transfer Polyester Label Material
3M 7816FL Thermal Transfer Polyester Label Materials
3M 7816 Thermal Transfer Polyester Label Materials
3M 7813 Thermal Transfer Polyester Label Material
3M 7810 Thermal Transfer Polyester Label Material

PMM33735 / 168482

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.