MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 7816 Thermal Transfer Polyester Label Materials
Categories: Polymer; Adhesive

Material Notes: 3M™ Thermal Transfer Polyester Label Materials 7816, 7816FL and 7875 are durable polyester label stocks that offer excellent moisture resistance and thermal stability. These label products utilize 3M™ Adhesive 310 which is a firm adhesive which resists oozing and provides high strength on a variety of surfaces including high surface energy (HSE) plastics and metals.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 20.3 microns0.800 milAdhesive
 50.8 microns2.00 milFacestock
 81.3 microns3.20 milLiner
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.05478 kN/m0.3125 pliLD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.0877 kN/m0.500 pliLD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.131 kN/m0.750 pliLD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.175 kN/m1.00 pliPolypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.175 kN/m1.00 pliHD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.1972 kN/m1.125 pliPolypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.1972 kN/m1.125 pliPolypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.219 kN/m1.25 pliLD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.219 kN/m1.25 pliHD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.219 kN/m1.25 pliHD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.219 kN/m1.25 pliLD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.2410 kN/m1.375 pliLD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.263 kN/m1.50 pliHD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.263 kN/m1.50 pliPolypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.263 kN/m1.50 pliLD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.29582 kN/m1.6875 pliPolypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.29582 kN/m1.6875 pliHD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.3287 kN/m1.875 pliHD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.3287 kN/m1.875 pliPolypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.351 kN/m2.00 pliLD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.351 kN/m2.00 pliPolycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.351 kN/m2.00 pliGlass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.36156 kN/m2.0625 pliHD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.3725 kN/m2.125 pliGlass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.38347 kN/m2.1875 pliStainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.38347 kN/m2.1875 pliPolypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.38347 kN/m2.1875 pliHD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.40538 kN/m2.3125 pliPolycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.4163 kN/m2.375 pliPolypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.438 kN/m2.50 pliPolycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.44921 kN/m2.5625 pliStainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.44921 kN/m2.5625 pliPolycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.4602 kN/m2.625 pliGlass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.47112 kN/m2.6875 pliStainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.47112 kN/m2.6875 pliPolycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.5040 kN/m2.875 pliStainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.5040 kN/m2.875 pliStainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.51494 kN/m2.9375 pliPolycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.51494 kN/m2.9375 pliGlass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.55877 kN/m3.1875 pliStainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.570 kN/m3.25 pliGlass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.570 kN/m3.25 pliPolycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.657 kN/m3.75 pliStainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.6793 kN/m3.875 pliPolycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.7231 kN/m4.125 pliGlass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.745 kN/m4.25 pliGlass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.745 kN/m4.25 pliGlass, 180° Peel, Conditioned for 3 days at 70°C; ASTM D3330
 0.8108 kN/m4.625 pliStainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 10.0 °C>= 50.0 °FApplication
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive Type310 Acrylic
Liner55# Densified kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 7222/7865 Thermal Transfer Polyester Label Material
3M 7816FL Thermal Transfer Polyester Label Materials
3M 7813 Thermal Transfer Polyester Label Material
3M 7810 Thermal Transfer Polyester Label Material
3M 7350FL Thermal Transfer Polyester Label Material

PMM33739 / 168486

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.