MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M 7247 Thermal Transfer Polyester with TT3 Matte Topcoating Label Material
Categories: Polymer; Adhesive

Material Notes: 3M™ Thermal Transfer Polyester Label Materials offer supreme image durability in harsh environments. The polyester label stock utilizes 3M™ Adhesive 350, which is designed to permanently bond to high and low surface energy plastics, textured and contoured surfaces, powder coatings and slightly oily metals

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 45.7 microns1.80 milAdhesive
 55.9 microns2.20 milFacestock
 55.9 microns2.20 milLiner
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.394 kN/m2.25 pliHDPE, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 0.40538 kN/m2.3125 pliHDPE, 90° Peel, Initial 20 min dwell at RT; FTM 2
 0.5040 kN/m2.875 pliLDPE, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 0.5040 kN/m2.875 pliHDPE, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 0.53686 kN/m3.0625 pliPolypropylene, 90° Peel, Initial 20 min dwell at RT; FTM 2
 0.53686 kN/m3.0625 pliLDPE, 90° Peel, Initial 20 min dwell at RT; FTM 2
 0.570 kN/m3.25 pliLDPE, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 0.62451 kN/m3.5625 pliAluminum, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 0.62451 kN/m3.5625 pliPowder Coating, 90° Peel, Initial 20 min dwell at RT; FTM 2
 0.6355 kN/m3.625 pliPolypropylene, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 0.66833 kN/m3.8125 pliPhenolic, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 0.66833 kN/m3.8125 pliPhenolic, 90° Peel, Initial 20 min dwell at RT; FTM 2
 0.6793 kN/m3.875 pliAluminum, 90° Peel, Initial 20 min dwell at RT; FTM 2
 0.6793 kN/m3.875 pliABS, 90° Peel, Initial 20 min dwell at RT; FTM 2
 0.6793 kN/m3.875 pliPolystyrene, 90° Peel, Initial 20 min dwell at RT; FTM 2
 0.701 kN/m4.00 pliPolycarbonate, 90° Peel, Initial 20 min dwell at RT; FTM 2
 0.7231 kN/m4.125 pliPolypropylene, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 0.73407 kN/m4.1875 pliPolycarbonate, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 0.73407 kN/m4.1875 pliStainless Steel, 90° Peel, Initial 20 min dwell at RT; FTM 2
 0.745 kN/m4.25 pliPolystyrene, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 0.745 kN/m4.25 pliPolystyrene, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 0.745 kN/m4.25 pliABS, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 0.75598 kN/m4.3125 pliPowder Coating, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 0.789 kN/m4.50 pliStainless Steel, 90° Peel, Conditioned for 3 days at -40°C; FTM 2
 0.8108 kN/m4.625 pliPolycarbonate, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 0.84363 kN/m4.8125 pliPhenolic, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 0.877 kN/m5.00 pliABS, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 0.90937 kN/m5.1875 pliPowder Coating, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 0.93128 kN/m5.3125 pliAluminum, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 1.0847 kN/m6.1875 pliStainless Steel, 90° Peel, Ultimate Adhesion 72 hrs dwell at 21°C; FTM 2
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive Type350 Acrylic
Liner40# White Densified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 7222/7865 Thermal Transfer Polyester Label Material
3M 7816FL Thermal Transfer Polyester Label Materials
3M 7816 Thermal Transfer Polyester Label Materials
3M 7813 Thermal Transfer Polyester Label Material
3M 7810 Thermal Transfer Polyester Label Material

PMM33735 / 168482

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.