MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Acetone (CH3COCH3; 2-Propanone; Dimethyl Ketone)
Categories: Fluid; Solvent

Key Words: CH3COCH3
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.7899 g/cc
@Temperature 20.0 °C
Viscosity 0.306 cP
@Temperature 25.0 °C
 0.317 cP
@Temperature 20.0 °C
Dynamic Viscosity
Molecular Weight 58.08 g/mol
Vapor Pressure 0.09869 atm
@Temperature 1.30 °C
 184.862 torr
@Temperature 20.0 °C
Surface Tension 23.46 dynes/cmat 25°C; Gamma
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 46.385 atm
Critical Temperature 234.98 °C
Critical Density 0.278 g/cc
Critical Molar Volume 209 cm³/mol
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 20.7
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 99.35 J/gEnthalpy of fusion at normal melting point
Heat of Vaporization 501 J/gEnthalpy of vaporization at normal boiling temperature
 501.4 J/g
Specific Heat Capacity 2.15 J/g-°C
 1.263 J/g-°C
@Temperature 25.0 °C
Vapor
Thermal Conductivity 0.0115 W/m-K
@Temperature 26.9 °C
gas at saturation vapor pressure
 0.161 W/m-K
@Temperature 25.0 °C
 0.0202 W/m-K
@Pressure 0.100 MPa,
Temperature 127 °C
gas
 0.0306 W/m-K
@Pressure 0.100 MPa,
Temperature 227 °C
gas
 0.0427 W/m-K
@Pressure 0.100 MPa,
Temperature 327 °C
gas
Melting Point -94.7 °CAt atmospheric pressure (760 torr)
Boiling Point 56.05 °C
@Pressure 0.101 MPa
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.3588
@Temperature 20.0 °C,
Wavelength 589.3 nm
Na D line
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.6513
Antoine's Vapor Pressure B Parameter2940.46
Antoine's Vapor Pressure C Parameter-35.93
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)67-64-1
Chemical FormulaCH3COCH3
Critical Compressibility (Zc)0.232
Dipole moment (p/C.m)9.673E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A367.25
Dynamic Viscosity Parameter B209.68
Henry's Law Constant (atm m3/mol)3.88E-05
Molar Heat Capacity (298K)73.35 J/mol-K
Molar Heat Capacity of Vapor a Parameter6.2969
Molar Heat Capacity of Vapor b Parameter0.2604
Molar Heat Capacity of Vapor c Parameter-0.0001252
Molar Heat Capacity of Vapor d Parameter2.036E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UV cut-off (nm)330

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Methanol (CH3OH; Methyl Alcohol)
Nitric Acid, HNO3
Honeywell Acetone B&J Brand® For Pesticide Residue Analysis
Hydrogen Chloride, HCl
Honeywell Acetone Laboratory Plus

VORG001 / 74512

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.