MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Methanol (CH3OH; Methyl Alcohol)
Categories: Fluid; Solvent

Key Words: CH3OH
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.7914 g/cc
@Temperature 20.0 °C
0.02859 lb/in³
@Temperature 68.0 °F
Viscosity  0.544 cP
@Temperature 25.0 °C
0.544 cP
@Temperature 77.0 °F
 0.58 cP
@Temperature 20.0 °C
0.58 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 32.04 g/mol32.04 g/mol
Vapor Pressure  0.1000 bar
@Temperature 15.2 °C
75.00 torr
@Temperature 59.4 °F
 0.130 bar
@Temperature 20.0 °C
97.3 torr
@Temperature 68.0 °F
Surface Tension  22.07 dynes/cm
@Temperature 25.0 °C
22.07 dynes/cm
@Temperature 77.0 °F
Gamma
 22.3 dynes/cm
@Temperature 20.0 °C
22.3 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 80.8400 bar60635.0 torr
Critical Temperature 239.38 °C462.88 °F
Critical Density 0.274 g/cc0.00990 lb/in³
Critical Molar Volume 117 cm³/mol7.14 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 32.6332.63
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 100.3 J/g43.17 BTU/lbEnthalpy of fusion at normal melting point
Heat of Vaporization 1099 J/g472.7 BTU/lbEnthalpy of vaporization at normal boiling temperature
Specific Heat Capacity 2.542 J/g-°C0.6076 BTU/lb-°F
 1.367 J/g-°C
@Temperature 25.0 °C
0.3267 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.200 W/m-K
@Temperature 25.0 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
 0.0262 W/m-K
@Pressure 0.100 MPa,
Temperature 127 °C
0.182 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 260 °F
gas
 0.0386 W/m-K
@Pressure 0.100 MPa,
Temperature 227 °C
0.268 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 440 °F
gas
 0.0530 W/m-K
@Pressure 0.100 MPa,
Temperature 327 °C
0.368 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 620 °F
gas
Melting Point -97.53 °C-143.6 °FAt atmospheric pressure (760 torr)
Boiling Point 64.6 °C
@Pressure 0.101 MPa
148 °F
@Pressure 14.7 psi
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.3288
@Temperature 20.0 °C,
Wavelength 589.3 nm
1.3288
@Temperature 68.0 °F,
Wavelength 589.3 nm
Na D line
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter18.5875
Antoine's Vapor Pressure B Parameter3626.55
Antoine's Vapor Pressure C Parameter-34.29
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)67-56-1
Chemical FormulaCH4O
Critical Compressibility (Zc)0.224
Dipole moment (p/C.m)5.671E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A555.3
Dynamic Viscosity Parameter B260.64
Henry's Law Constant (atm m3/mol)4.45E-06
Molar Heat Capacity (298K)43.812 J/mol-K
Molar Heat Capacity of Vapor a Parameter21.1376
Molar Heat Capacity of Vapor b Parameter0.0709
Molar Heat Capacity of Vapor c Parameter2.585E-05
Molar Heat Capacity of Vapor d Parameter-2.85E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1230
UV cut-off (nm)210

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Acetone (CH3COCH3; 2-Propanone; Dimethyl Ketone)
Water, H2O
Ethanol (CH3CH2OH; Ethyl Alcohol)
3M Fluorinert™ FC-72 Electronic Liquid
3M 4604 Silicone Rubber Termination Kit

VORG029 / 74540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.