MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Methanol (CH3OH; Methyl Alcohol)
Categories: Fluid; Solvent

Key Words: CH3OH
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.7914 g/cc
@Temperature 20.0 °C
Viscosity 0.544 cP
@Temperature 25.0 °C
 0.58 cP
@Temperature 20.0 °C
Dynamic Viscosity
Molecular Weight 32.04 g/mol
Vapor Pressure 0.09869 atm
@Temperature 15.2 °C
 97.3 torr
@Temperature 20.0 °C
Surface Tension 22.07 dynes/cm
@Temperature 25.0 °C
Gamma
 22.3 dynes/cm
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 79.7829 atm
Critical Temperature 239.38 °C
Critical Density 0.274 g/cc
Critical Molar Volume 117 cm³/mol
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 32.63
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 100.3 J/gEnthalpy of fusion at normal melting point
Heat of Vaporization 1099 J/gEnthalpy of vaporization at normal boiling temperature
Specific Heat Capacity 2.542 J/g-°C
 1.367 J/g-°C
@Temperature 25.0 °C
Vapor
Thermal Conductivity 0.200 W/m-K
@Temperature 25.0 °C
 0.0262 W/m-K
@Pressure 0.100 MPa,
Temperature 127 °C
gas
 0.0386 W/m-K
@Pressure 0.100 MPa,
Temperature 227 °C
gas
 0.0530 W/m-K
@Pressure 0.100 MPa,
Temperature 327 °C
gas
Melting Point -97.53 °CAt atmospheric pressure (760 torr)
Boiling Point 64.6 °C
@Pressure 0.101 MPa
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.3288
@Temperature 20.0 °C,
Wavelength 589.3 nm
Na D line
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter18.5875
Antoine's Vapor Pressure B Parameter3626.55
Antoine's Vapor Pressure C Parameter-34.29
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)67-56-1
Chemical FormulaCH4O
Critical Compressibility (Zc)0.224
Dipole moment (p/C.m)5.671E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A555.3
Dynamic Viscosity Parameter B260.64
Henry's Law Constant (atm m3/mol)4.45E-06
Molar Heat Capacity (298K)43.812 J/mol-K
Molar Heat Capacity of Vapor a Parameter21.1376
Molar Heat Capacity of Vapor b Parameter0.0709
Molar Heat Capacity of Vapor c Parameter2.585E-05
Molar Heat Capacity of Vapor d Parameter-2.85E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1230
UV cut-off (nm)210

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Acetone (CH3COCH3; 2-Propanone; Dimethyl Ketone)
Water, H2O
Ethanol (CH3CH2OH; Ethyl Alcohol)
3M Fluorinert™ FC-72 Electronic Liquid
3M 4604 Silicone Rubber Termination Kit

VORG029 / 74540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.