MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Hydrogen Chloride, HCl
Categories: Ceramic; Halide; Fluid

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.00149 g/cc0.0000538 lb/in³Gas
Molecular Weight 36.461 g/mol36.461 g/mol
 
Electrical PropertiesMetricEnglishComments
Magnetic Susceptibility -0.0000226-0.0000226cm^3/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 54.9 J/g23.6 BTU/lb
Thermal Conductivity  0.0145 W/m-K
@Pressure 0.100 MPa,
Temperature 26.9 °C
0.101 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 80.3 °F
gas
 0.0195 W/m-K
@Pressure 0.100 MPa,
Temperature 127 °C
0.135 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 260 °F
gas
 0.0240 W/m-K
@Pressure 0.100 MPa,
Temperature 227 °C
0.167 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 440 °F
gas
 0.0281 W/m-K
@Pressure 0.100 MPa,
Temperature 327 °C
0.195 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 620 °F
gas
Melting Point -114.17 °C-173.51 °F
Boiling Point -85.0 °C-121 °F
 
Descriptive Properties
CAS Number7647-01-0

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sulfuric Acid, H2SO4
Potassium Hydroxide, KOH
Ammonium Fluoride, NH4F
Hydrogen Fluoride, HF
Hydrogen Peroxide, H2O2

EINOR0316 / 3445

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.