MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hydrogen Fluoride, HF
Categories: Fluid

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.967 g/cc
@Temperature 20.0 °C
0.0349 lb/in³
@Temperature 68.0 °F
Viscosity 0.199 cP
@Temperature 20.0 °C
0.199 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 20.006 g/mol20.006 g/mol
Vapor Pressure 1.03008 bar
@Temperature 20.0 °C
772.624 torr
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 64.8 bar48600 torr
Critical Temperature 188 °C370 °F
Critical Density 0.290 g/cc0.0105 lb/in³
Critical Molar Volume 69.0 cm³/mol4.21 in³/mol
 
Electrical PropertiesMetricEnglishComments
Magnetic Susceptibility -0.00000860-0.00000860cm^3/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 228.9 J/g98.47 BTU/lb
Heat of Vaporization 334.6 J/g143.9 BTU/lb
Specific Heat Capacity 1.456 J/g-°C
@Temperature 25.0 °C
0.3480 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.431 W/m-K
@Temperature 20.0 °C
2.99 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -83.35 °C-118.0 °F
Boiling Point 19.6 °C67.3 °F
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter17.6958
Antoine's Vapor Pressure B Parameter3404.49
Antoine's Vapor Pressure C Parameter15.06
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS Number7664-39-3
CAS registry number (CARN)7664-39-3
Chemical FormulaHF
Critical Compressibility (Zc)0.12
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A194.7
Dynamic Viscosity Parameter B145.31
Molar Heat Capacity (298K)29.124 J/mol-K
Molar Heat Capacity of Vapor a Parameter29.0411
Molar Heat Capacity of Vapor b Parameter0.0007
Molar Heat Capacity of Vapor c Parameter-2.031E-06
Molar Heat Capacity of Vapor d Parameter2.502E-09
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sulfuric Acid, H2SO4
Hydrogen Chloride, HCl
Hydrogen Peroxide, H2O2
Ammonium Fluoride, NH4F
Rhenium, Re; Deformed

EINOR0317 / 3446

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.