MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik Chromflex 12C27 Strip steel
Categories: Metal; Ferrous Metal; Alloy Steel; Martensitic

Material Notes: Sandvik Chromflex is a family of hardened and tempered martensitic chromium steels characterized by:
  • High strength combined with good shape
  • High standard of surface finish
  • Close dimensional tolerances
  • Freedom from internal stresses
  • Low content of non-metallic inclusions
Each of the four grades in the Sandvik Chromflex family has its own distinguishing characteristics: Good edge properties and high toughness for heavy gauges

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.70 g/cc0.278 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  1800 MPa
@Thickness 0.500 - 1.00 mm
261000 psi
@Thickness 0.0197 - 0.0394 in
 1900 MPa
@Thickness 0.300 - 0.500 mm
276000 psi
@Thickness 0.0118 - 0.0197 in
Tensile Strength, Yield  1200 MPa
@Strain 0.01 %,
Thickness 0.500 - 1.00 mm
174000 psi
@Strain 0.01 %,
Thickness 0.0197 - 0.0394 in
Elastic limit
 1300 MPa
@Strain 0.01 %,
Thickness 0.300 - 0.500 mm
189000 psi
@Strain 0.01 %,
Thickness 0.0118 - 0.0197 in
Elastic limit
 1450 MPa
@Strain 0.2 %,
Thickness 0.500 - 1.00 mm
210000 psi
@Strain 0.2 %,
Thickness 0.0197 - 0.0394 in
 1550 MPa
@Strain 0.2 %,
Thickness 0.300 - 0.500 mm
225000 psi
@Strain 0.2 %,
Thickness 0.0118 - 0.0197 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.6 µm/m-°C
@Temperature 20.0 - 100 °C
5.89 µin/in-°F
@Temperature 68.0 - 212 °F
 11.1 µm/m-°C
@Temperature 20.0 - 200 °C
6.17 µin/in-°F
@Temperature 68.0 - 392 °F
 11.4 µm/m-°C
@Temperature 20.0 - 300 °C
6.33 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 J/g-°C0.110 BTU/lb-°F
Thermal Conductivity 24.0 W/m-K167 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.60 %0.60 %
Chromium, Cr 13.5 %13.5 %
Manganese, Mn 0.40 %0.40 %
Silicon, Si 0.40 %0.40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik Chromflex 13C26 Strip steel
Sandvik Chromflex 6C27 Strip steel
Sandvik Chromflex 7C27Mo2 Strip steel
Sandvik Sanprint RP Strip steel
Sandvik Sanprint EP Strip steel

NSANDV5209 / 199773

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.