MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik Sanprint RP Strip steel
Categories: Metal; Ferrous Metal; Alloy Steel; Martensitic

Material Notes: Sandvik Sanprint RP is a hardened and tempered carbon steel used for printing doctor blade applications. The grade is a standard martensitic steel, suitable for nonwater based inks and is characterized by:
  • High wear resistance
  • Good straightness
  • Good dimensional tolerances
  • Excellent edge finish

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers  535 - 585
@Thickness 0.305 mm
535 - 585
@Thickness 0.0120 in
 550 - 600
@Thickness 0.254 mm
550 - 600
@Thickness 0.0100 in
 565 - 615
@Thickness 0.203 mm
565 - 615
@Thickness 0.00799 in
 575 - 625
@Thickness 0.152 mm
575 - 625
@Thickness 0.00598 in
 585 - 635
@Thickness 0.0760 mm
585 - 635
@Thickness 0.00299 in
 585 - 635
@Thickness 0.102 mm
585 - 635
@Thickness 0.00402 in
Tensile Strength, Ultimate  1800 - 2000 MPa
@Thickness 0.305 mm
261000 - 290000 psi
@Thickness 0.0120 in
 1850 - 2050 MPa
@Thickness 0.254 mm
268000 - 297000 psi
@Thickness 0.0100 in
 1900 - 2100 MPa
@Thickness 0.203 mm
276000 - 305000 psi
@Thickness 0.00799 in
 1950 - 2150 MPa
@Thickness 0.152 mm
283000 - 312000 psi
@Thickness 0.00598 in
 2000 - 2200 MPa
@Thickness 0.0760 mm
290000 - 319000 psi
@Thickness 0.00299 in
 2000 - 2200 MPa
@Thickness 0.102 mm
290000 - 319000 psi
@Thickness 0.00402 in
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.0 %1.0 %
Chromium, Cr 0.20 %0.20 %
Manganese, Mn 0.45 %0.45 %
Silicon, Si 0.25 %0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik Chromflex 12C27 Strip steel
Sandvik Chromflex 13C26 Strip steel
Sandvik Chromflex 6C27 Strip steel
Sandvik Chromflex 7C27Mo2 Strip steel
Sandvik Sanprint EP Strip steel

NSANDV5221 / 199785

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.