Sandvik Sanprint EP is a hardened and tempered carbon steel used for printing doctor blade applications. The grade is a standard martensitic steel, particularly suitable for non waterbased and UV inks and is characterized by:- Very high wear resistance
- Good straightness
- Excellent edge finish
- Good dimensional tolerances
Information provided by Sandvik |