MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Sanprint EP Strip steel
Categories: Metal; Ferrous Metal; Alloy Steel; Martensitic

Material Notes: Sandvik Sanprint EP is a hardened and tempered carbon steel used for printing doctor blade applications. The grade is a standard martensitic steel, particularly suitable for non waterbased and UV inks and is characterized by:
  • Very high wear resistance
  • Good straightness
  • Excellent edge finish
  • Good dimensional tolerances

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 535 - 585
@Thickness 0.305 mm
 550 - 600
@Thickness 0.254 mm
 565 - 615
@Thickness 0.203 mm
 575 - 625
@Thickness 0.152 mm
 585 - 635
@Thickness 0.0760 mm
 585 - 635
@Thickness 0.102 mm
Tensile Strength, Ultimate 1800 - 2000 MPa
@Thickness 0.305 mm
 1850 - 2050 MPa
@Thickness 0.254 mm
 1900 - 2100 MPa
@Thickness 0.203 mm
 1950 - 2150 MPa
@Thickness 0.152 mm
 2000 - 2200 MPa
@Thickness 0.0760 mm
 2000 - 2200 MPa
@Thickness 0.102 mm
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.0 %
Chromium, Cr 1.4 %
Manganese, Mn 0.30 %
Silicon, Si 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Chromflex 12C27 Strip steel
Sandvik Sanprint RP Strip steel
Sandvik Chromflex 13C26 Strip steel
Sandvik Chromflex 6C27 Strip steel
Sandvik Chromflex 7C27Mo2 Strip steel

NSANDV5219 / 199783

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.