MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Rogers Corporation TMM® TMM10 Ceramic Thermoset Polymer Composite
Categories: Polymer; Thermoset

Material Notes: TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical properties of TMM laminates combine many of the benefits of both ceramic and traditional PTFE microwave circuit laminates, without requiring the specialized production techniques common to these materials.

Features:

  • Wide range of dielectric constants. Ideal for single material systems on a wide variety of applications.
  • Excellent mechanical properties. Resists creep and cold flow.
  • Exceptionally low thermal coefficient of dielectric constant.
  • Coefficient of thermal expansion matched to copper. High reliability of plated through holes.
  • Resistant to process chemicals. No damage to material during fabrication and assembly processes.
  • Thermoset resin for reliable wirebonding. No specialized production techniques required. TMM 10 and 10i laminates can replace alumina substrates.
  • Lead-free process compatible

Typical Applications:

  • RF and Microwave Circuitry
  • Global Positioning Systems Antennas
  • Power Amplifiers and Combiners
  • Patch Antennas
  • Filters and Coupler
  • Dielectric Polarizers and Lenses
  • Satellite Communication Systems
  • Chip Testers

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.77 g/ccASTM D792
Water Absorption 0.090 %
@Thickness 1.27 mm
D/48/50; ASTM D570
 0.20 %
@Thickness 3.17 mm
D/48/50; ASTM D570
Thickness 15.0 - 500 milRange of Standard Thicknesses
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 93.9 MPaX, Y direction; Condition A; ASTM D790
Flexural Modulus 12300 MPaX, Y direction; Condition A; ASTM D790
Izod Impact, Notched 0.430 ft-lb/inX, Y direction; ASTM D256A
Peel Strength 5.00 pliX, Y direction; after solder float 1 oz. EDC; IPC-TM-650 2.4.8
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+14 ohm-cmASTM D257
Surface Resistance 4.00e+13 ohmASTM D257
Insulation Resistance >= 2.00e+12 ohmC/96/60/95; ASTM D257
Dielectric Constant 8.97 - 9.43
@Frequency 1e+10 Hz
Z direction; IPC-TM-650 2.5.5.5
Dissipation Factor 0.0022
@Frequency 1e+10 Hz
Z direction; IPC-TM-650, 2.5.5.5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µm/m-°C
@Temperature 0.000 - 140 °C
Z-Direction; ASTM D3386
 21.0 µm/m-°C
@Temperature 0.000 - 140 °C
X-, Y-Direction; ASTM D3386
Specific Heat Capacity 0.740 J/g-°Ccalculated
Thermal Conductivity 1.76 W/m-K
@Temperature 80.0 °C
ASTM C518
Decomposition Temperature 425 °CTGA; ASTM D3850
 
Descriptive Properties
Thermal Coefficient of Dielectric Constant-38 ppm/°CIPC-TM-650 2.5.5.5; -55°C to 125°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Corporation TMM® TMM6 Ceramic Thermoset Polymer Composite
Rogers Corporation RO4450F Prepreg
Rogers Corporation RO4450B Prepreg
Rogers Corporation RO4003C Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil
Rogers Corporation RO3003 Ceramic-Filled PTFE Composite, High Frequency Circuit Material

PROGA982 / 138422

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.