MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Corporation RO3003 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Features and Benefits:Low dielectric loss - Laminates can be used in applications up to 77 GHz.
  • Excellent mechanical properties versus temperature - reliable stripline and multi-layer board constructions.
  • Uniform mechanical properties for a range of dielectric constants - ideal for multi-layer board designs with a range of dielectric constants and suitable for use with epoxy glass multi-layer board hybrid designs.
  • Stable dielectric constant versus temperature and frequency - ideal for band pass filters, microstrip patch antennas and voltage controlled oscillators
  • Low in-plane expansion coefficient (match to copper) - allows for more reliable surface mounted assemblies, ideal for applications sensitive to temperature change and excellent dimensional stability
  • Volume manufacturing process - Economical laminate pricing
  • Lead-free process compatible

    Typical Applications:

    • Automotive radar applications
    • Global positioning satellite antennas
    • Cellular telecommunications systems - power amplifiers and antennas
    • Patch antenna for wireless communications
    • Direct broadcast satellites
    • Datalink on cable systems
    • Remote meter readers
    • Power backplanes

    Information provided by Rogers Corporation.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 2.10 g/cc0.0759 lb/in³
    Water Absorption <= 0.10 %<= 0.10 %D24/23; IPC-TM-2.4.8
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Modulus 0.903 GPa131 ksiX, Y-Direction; ASTM D638
    Peel Strength 2.23 kN/m12.7 pliCopper; 1/2 oz. EDC After Solder Float; IPC-TM-650 2.4.8
     
    Electrical PropertiesMetricEnglishComments
    Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmCond. A; IPC 2.5.17.1
    Surface Resistance 1.00e+13 ohm1.00e+13 ohmCond. A; IPC 2.5.17.1
    Dielectric Constant  2.96 - 3.04
    @Frequency 1e+10 Hz
    2.96 - 3.04
    @Frequency 1e+10 Hz
    Clamped stripline, Z-direction; IPC-TM-650 2.5.5.5
     3.0
    @Frequency 8.00e+9 - 4.00e+10 Hz
    3.0
    @Frequency 8.00e+9 - 4.00e+10 Hz
    Differential Phase Length Method, Z-Direction
    Dissipation Factor 0.0013
    @Frequency 1e+10 Hz
    0.0013
    @Frequency 1e+10 Hz
    IPC-TM-650 2.5.5.5
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear  16.0 µm/m-°C
    @Temperature -55.0 - 288 °C
    8.89 µin/in-°F
    @Temperature -67.0 - 550 °F
    Y-Direction; ASTM D3386-94
     17.0 µm/m-°C
    @Temperature -55.0 - 288 °C
    9.44 µin/in-°F
    @Temperature -67.0 - 550 °F
    X-Direction; ASTM D3386-94
     25.0 µm/m-°C
    @Temperature -55.0 - 288 °C
    13.9 µin/in-°F
    @Temperature -67.0 - 550 °F
    Z-Direction; ASTM D3386-94
    Specific Heat Capacity 0.900 J/g-°C0.215 BTU/lb-°FCalculated
    Thermal Conductivity 0.500 W/m-K
    @Temperature 80.0 °C
    3.47 BTU-in/hr-ft²-°F
    @Temperature 176 °F
    Z Direction; ASTM C518
    Decomposition Temperature 500 °C932 °FTGA; ASTM D3850
    Flammability, UL94 V-0V-0
     
    Descriptive Properties
    Dimensional Stability0.01 mm/mASTM D257, Cond. A; X, Y-direction
    Thermal Coefficient of Dielectric Constant13 ppm/°CIPC-TM-650 2.5.5.5; 10 GHz; 0°C to 100°C; Z-Direction

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Rogers Corporation RO3006 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
    Overview - Alumina, 96%, Al2O3
    Rogers Corporation RO3010 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
    Rogers Corporation RO3035 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
    Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate

    PROGA946 / 138386

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.