MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Styroclear GH 62 SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styroclear GH 62 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warpage resistance for general injection molding applications. Styroclear GH 62 may be suitable for conventional thermoplastics processing technologies such as injection molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccISO 1183
Water Absorption 0.070 %ISO 62
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM Test
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 69ASTM Test
Tensile Strength, Yield 28.0 MPa2 in/min; ASTM Test
Elongation at Break 100 %2 in/min; ASTM Test
Tensile Modulus 1730 MPa2 in/min; ASTM Test
Flexural Strength 31.0 MPaASTM Test
Flexural Modulus 1480 MPaASTM Test
Dart Drop, Total Energy 5.00 JASTM Test
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °CASTM Test
Vicat Softening Point 91.0 °CRate "B" Loading 1 (120 degC/h 10N); ASTM Test
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 92 %
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 250 °CInjection Molding
Mold Temperature 30.0 - 50.0 °CInjection Molding
 
Descriptive Properties
ColorClear
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Styroclear GH 58 SBC
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
INEOS Styrolution Styrolux® BX6400 SBC
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Overview of materials for Styrene-Butadiene Copolymer, SBC

PBASF9026 / 84790

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.