MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Styrene-Butadiene Copolymer, SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.848 - 7.98 g/cc0.0306 - 0.288 lb/in³Average value: 1.17 g/cc Grade Count:88
Water Absorption 0.0700 - 0.0900 %0.0700 - 0.0900 %Average value: 0.0809 % Grade Count:11
Water Absorption at Saturation 0.0700 %0.0700 %Average value: 0.0700 % Grade Count:20
pH 7.00 - 11.37.00 - 11.3Average value: 9.86 Grade Count:4
Water Vapor Transmission 54.3 - 93.1 g/m²/day3.50 - 6.00 g/100 in²/dayAverage value: 77.6 g/m²/day Grade Count:3
Oxygen Transmission Rate 27.2 - 6520 cc/m²/day1.75 - 420 cc/100 in²/dayAverage value: 2820 cc/m²/day Grade Count:5
Viscosity 150 - 2000 cP150 - 2000 cPAverage value: 713 cP Grade Count:4
Linear Mold Shrinkage 0.00200 - 0.0370 cm/cm0.00200 - 0.0370 in/inAverage value: 0.00977 cm/cm Grade Count:31
Melt Flow 1.00 - 76.0 g/10 min1.00 - 76.0 g/10 minAverage value: 12.4 g/10 min Grade Count:66
Surface Tension 31.0 - 40.0 dynes/cm31.0 - 40.0 dynes/cmAverage value: 35.5 dynes/cm Grade Count:3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9.00 - 97.09.00 - 97.0Average value: 63.6 Grade Count:33
Hardness, Shore D 34.0 - 91.034.0 - 91.0Average value: 63.9 Grade Count:48
Tensile Strength, Ultimate 1.61 - 27.6 MPa234 - 4000 psiAverage value: 11.6 MPa Grade Count:39
Film Tensile Strength at Yield, MD 20.0 - 34.5 MPa2900 - 5000 psiAverage value: 27.4 MPa Grade Count:4
Film Tensile Strength at Yield, TD 16.0 - 70.0 MPa2320 - 10200 psiAverage value: 30.8 MPa Grade Count:4
Tensile Strength, Yield 1.03 - 45.5 MPa149 - 6600 psiAverage value: 23.1 MPa Grade Count:59
Film Elongation at Break, MD 65.0 - 260 %65.0 - 260 %Average value: 163 % Grade Count:5
Film Elongation at Break, TD 80.0 - 260 %80.0 - 260 %Average value: 179 % Grade Count:5
Elongation at Break 2.50 - 1300 %2.50 - 1300 %Average value: 338 % Grade Count:79
Elongation at Yield 1.50 - 5.00 %1.50 - 5.00 %Average value: 2.51 % Grade Count:25
Modulus of Elasticity 0.0689 - 2.90 GPa10.0 - 421 ksiAverage value: 1.35 GPa Grade Count:32
Flexural Yield Strength 4.00 - 75.0 MPa580 - 10900 psiAverage value: 33.7 MPa Grade Count:53
Flexural Modulus 0.140 - 3.00 GPa20.3 - 435 ksiAverage value: 1.42 GPa Grade Count:54
Resilience 33.0 - 43.033.0 - 43.0Average value: 38.6 Grade Count:9
Secant Modulus, MD 0.696 - 1.27 GPa101 - 185 ksiAverage value: 0.956 GPa Grade Count:4
Secant Modulus, TD 0.469 - 1.60 GPa68.0 - 232 ksiAverage value: 0.884 GPa Grade Count:4
Izod Impact, Notched 0.198 J/cm - NB0.371 ft-lb/in - NBAverage value: 0.662 J/cm Grade Count:26
Izod Impact, Notched (ISO) 2.30 kJ/m² - NB1.09 ft-lb/in² - NBAverage value: 3.31 kJ/m² Grade Count:12
 2.00 - 4.00 kJ/m²
@Temperature -30.0 - -30.0 °C
0.952 - 1.90 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 2.92 kJ/m² Grade Count:6
Charpy Impact Unnotched 1.30 J/cm² - NB6.19 ft-lb/in² - NBAverage value: 5.17 J/cm² Grade Count:26
 2.00 J/cm² - NB
@Temperature -30.0 - -30.0 °C
9.52 ft-lb/in² - NB
@Temperature -22.0 - -22.0 °F
Average value: 2.50 J/cm² Grade Count:5
Charpy Impact, Notched 0.100 J/cm² - NB0.476 ft-lb/in² - NBAverage value: 1.55 J/cm² Grade Count:30
 0.200 - 0.200 J/cm²
@Temperature -30.0 - -30.0 °C
0.952 - 0.952 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 2.79 J/cm² Grade Count:3
Dart Drop, Total Energy 0.600 - 40.0 J0.443 - 29.5 ft-lbAverage value: 11.3 J Grade Count:9
Instrumented Impact Total Energy 28.2 - 37.6 J20.8 - 27.7 ft-lbAverage value: 34.5 J Grade Count:3
Tear Strength 6.30 - 104 kN/m35.9 - 593 pliAverage value: 34.6 kN/m Grade Count:26
Elmendorf Tear Strength MD 9.10 - 660 g9.10 - 660 gAverage value: 337 g Grade Count:4
Elmendorf Tear Strength TD 1.50 - 816 g1.50 - 816 gAverage value: 415 g Grade Count:4
Dart Drop Test 325 - 590 g0.717 - 1.30 lbAverage value: 460 g Grade Count:4
Compression Set 8.00 - 43.0 %8.00 - 43.0 %Average value: 24.3 % Grade Count:13
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+7 - 1.00e+15 ohm-cm1.00e+7 - 1.00e+15 ohm-cmAverage value: 7.28e+14 ohm-cm Grade Count:11
Surface Resistance 1.00e+8 - 1.00e+15 ohm1.00e+8 - 1.00e+15 ohmAverage value: 7.36e+14 ohm Grade Count:11
Dielectric Constant 2.502.50Average value: 2.50 Grade Count:8
Dissipation Factor 0.000300 - 0.0008000.000300 - 0.000800Average value: 0.000533 Grade Count:8
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:8
 
Thermal PropertiesMetricEnglishComments
CTE, linear 59.4 - 90.0 µm/m-°C33.0 - 50.0 µin/in-°FAverage value: 75.0 µm/m-°C Grade Count:14
Deflection Temperature at 0.46 MPa (66 psi) 55.0 - 82.0 °C131 - 180 °FAverage value: 71.7 °C Grade Count:20
Deflection Temperature at 1.8 MPa (264 psi) 39.0 - 83.0 °C102 - 181 °FAverage value: 63.6 °C Grade Count:45
Vicat Softening Point 35.0 - 99.0 °C95.0 - 210 °FAverage value: 73.2 °C Grade Count:58
Brittleness Temperature -64.0 - -50.0 °C-83.2 - -58.0 °FAverage value: -56.0 °C Grade Count:6
Flammability, UL94 HB - V-0HB - V-0Grade Count:10
Oxygen Index 27.0 %27.0 %Average value: 27.0 % Grade Count:4
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.56 - 1.581.56 - 1.58Average value: 1.57 Grade Count:18
Haze 0.200 - 28.0 %0.200 - 28.0 %Average value: 2.67 % Grade Count:37
Gloss 125 - 162 %125 - 162 %Average value: 143 % Grade Count:9
Transmission, Visible 77.0 - 99.0 %77.0 - 99.0 %Average value: 90.1 % Grade Count:52
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 232 °C356 - 450 °FAverage value: 213 °C Grade Count:12
Nozzle Temperature 190 - 200 °C374 - 392 °FAverage value: 195 °C Grade Count:4
Melt Temperature 163 - 250 °C325 - 482 °FAverage value: 207 °C Grade Count:30
Mold Temperature 10.0 - 50.0 °C50.0 - 122 °FAverage value: 36.6 °C Grade Count:21
Drying Temperature 60.0 - 76.7 °C140 - 170 °FAverage value: 68.3 °C Grade Count:6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
Overview of materials for Styrene/Butadiene/Styrene (SBS)
Overview of materials for Cyclo Olefin Polymer
Overview of materials for Styrenic Elastomer (TES)
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber

O4980 / 78448

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.