MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Styrene-Butadiene Copolymer, SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.848 - 7.98 g/ccAverage value: 1.17 g/cc Grade Count:88
Water Absorption 0.0700 - 0.0900 %Average value: 0.0809 % Grade Count:11
Water Absorption at Saturation 0.0700 %Average value: 0.0700 % Grade Count:20
pH 7.00 - 11.3Average value: 9.86 Grade Count:4
Water Vapor Transmission 54.3 - 93.1 g/m²/dayAverage value: 77.6 g/m²/day Grade Count:3
Oxygen Transmission Rate 27.2 - 6520 cc/m²/dayAverage value: 2820 cc/m²/day Grade Count:5
Viscosity 150 - 2000 cPAverage value: 713 cP Grade Count:4
Linear Mold Shrinkage 0.00200 - 0.0370 cm/cmAverage value: 0.00977 cm/cm Grade Count:31
Melt Flow 1.00 - 76.0 g/10 minAverage value: 12.4 g/10 min Grade Count:66
Surface Tension 31.0 - 40.0 dynes/cmAverage value: 35.5 dynes/cm Grade Count:3
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 9.00 - 97.0Average value: 63.6 Grade Count:33
Hardness, Shore D 34.0 - 91.0Average value: 63.9 Grade Count:48
Tensile Strength, Ultimate 1.61 - 27.6 MPaAverage value: 11.6 MPa Grade Count:39
Film Tensile Strength at Yield, MD 20.0 - 34.5 MPaAverage value: 27.4 MPa Grade Count:4
Film Tensile Strength at Yield, TD 16.0 - 70.0 MPaAverage value: 30.8 MPa Grade Count:4
Tensile Strength, Yield 1.03 - 45.5 MPaAverage value: 23.1 MPa Grade Count:59
Film Elongation at Break, MD 65.0 - 260 %Average value: 163 % Grade Count:5
Film Elongation at Break, TD 80.0 - 260 %Average value: 179 % Grade Count:5
Elongation at Break 2.50 - 1300 %Average value: 338 % Grade Count:79
Elongation at Yield 1.50 - 5.00 %Average value: 2.51 % Grade Count:25
Modulus of Elasticity 0.0689 - 2.90 GPaAverage value: 1.35 GPa Grade Count:32
Flexural Yield Strength 4.00 - 75.0 MPaAverage value: 33.7 MPa Grade Count:53
Flexural Modulus 0.140 - 3.00 GPaAverage value: 1.42 GPa Grade Count:54
Resilience 33.0 - 43.0Average value: 38.6 Grade Count:9
Secant Modulus, MD 0.696 - 1.27 GPaAverage value: 0.956 GPa Grade Count:4
Secant Modulus, TD 0.469 - 1.60 GPaAverage value: 0.884 GPa Grade Count:4
Izod Impact, Notched 0.198 J/cm - NBAverage value: 0.662 J/cm Grade Count:26
Izod Impact, Notched (ISO) 2.30 kJ/m² - NBAverage value: 3.31 kJ/m² Grade Count:12
 2.00 - 4.00 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 2.92 kJ/m² Grade Count:6
Charpy Impact Unnotched 1.30 J/cm² - NBAverage value: 5.17 J/cm² Grade Count:26
 2.00 J/cm² - NB
@Temperature -30.0 - -30.0 °C
Average value: 2.50 J/cm² Grade Count:5
Charpy Impact, Notched 0.100 J/cm² - NBAverage value: 1.55 J/cm² Grade Count:30
 0.200 - 0.200 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 2.79 J/cm² Grade Count:3
Dart Drop, Total Energy 0.600 - 40.0 JAverage value: 11.3 J Grade Count:9
Instrumented Impact Total Energy 28.2 - 37.6 JAverage value: 34.5 J Grade Count:3
Tear Strength 6.30 - 104 kN/mAverage value: 34.6 kN/m Grade Count:26
Elmendorf Tear Strength MD 9.10 - 660 gAverage value: 337 g Grade Count:4
Elmendorf Tear Strength TD 1.50 - 816 gAverage value: 415 g Grade Count:4
Dart Drop Test 325 - 590 gAverage value: 460 g Grade Count:4
Compression Set 8.00 - 43.0 %Average value: 24.3 % Grade Count:13
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+7 - 1.00e+15 ohm-cmAverage value: 7.28e+14 ohm-cm Grade Count:11
Surface Resistance 1.00e+8 - 1.00e+15 ohmAverage value: 7.36e+14 ohm Grade Count:11
Dielectric Constant 2.50Average value: 2.50 Grade Count:8
Dissipation Factor 0.000300 - 0.000800Average value: 0.000533 Grade Count:8
Comparative Tracking Index 600 VAverage value: 600 V Grade Count:8
 
Thermal PropertiesOriginal ValueComments
CTE, linear 59.4 - 90.0 µm/m-°CAverage value: 75.0 µm/m-°C Grade Count:14
Deflection Temperature at 0.46 MPa (66 psi) 55.0 - 82.0 °CAverage value: 71.7 °C Grade Count:20
Deflection Temperature at 1.8 MPa (264 psi) 39.0 - 83.0 °CAverage value: 63.6 °C Grade Count:45
Vicat Softening Point 35.0 - 99.0 °CAverage value: 73.2 °C Grade Count:58
Brittleness Temperature -64.0 - -50.0 °CAverage value: -56.0 °C Grade Count:6
Flammability, UL94 HB - V-0Grade Count:10
Oxygen Index 27.0 %Average value: 27.0 % Grade Count:4
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.56 - 1.58Average value: 1.57 Grade Count:18
Haze 0.200 - 28.0 %Average value: 2.67 % Grade Count:37
Gloss 125 - 162 %Average value: 143 % Grade Count:9
Transmission, Visible 77.0 - 99.0 %Average value: 90.1 % Grade Count:52
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 232 °CAverage value: 213 °C Grade Count:12
Nozzle Temperature 190 - 200 °CAverage value: 195 °C Grade Count:4
Melt Temperature 163 - 250 °CAverage value: 207 °C Grade Count:30
Mold Temperature 10.0 - 50.0 °CAverage value: 36.6 °C Grade Count:21
Drying Temperature 60.0 - 76.7 °CAverage value: 68.3 °C Grade Count:6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
Overview of materials for Styrene/Butadiene/Styrene (SBS)
Overview of materials for Cyclo Olefin Polymer
Overview of materials for Styrenic Elastomer (TES)
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber

O4980 / 78448

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.