MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Styroclear GH 58 SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styroclear GH 58 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warpage resistance for general molding applications. Styroclear GH 58 may be suitable for conventional thermoplastics processing technologies such as injection molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183
Water Absorption 0.070 %0.070 %ISO 62
Melt Flow 16 g/10 min
@Load 5.00 kg,
Temperature 200 °C
16 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM Test
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7474ASTM Test
Tensile Strength, Yield 28.0 MPa4060 psi2 in/min; ASTM Test
Elongation at Break 43 %43 %2 in/min; ASTM Test
Tensile Modulus 1.68 GPa244 ksi2 in/min; ASTM Test
Flexural Strength 33.0 MPa4790 psiASTM Test
Flexural Modulus 1.50 GPa218 ksiASTM Test
Dart Drop, Total Energy 0.600 J0.443 ft-lbASTM Test
 
Electrical PropertiesMetricEnglishComments
Dissipation Factor  0.00030
@Frequency 1e+9 Hz
0.00030
@Frequency 1e+9 Hz
ASTM Data
 0.00080
@Frequency 1e+6 Hz
0.00080
@Frequency 1e+6 Hz
ASTM Data
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C153 °FASTM Test
Vicat Softening Point 90.0 °C194 °FRate "B" Loading 1 (120 degC/h 10N); ASTM Test
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 235 °C356 - 455 °FInjection Molding
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °FInjection Molding
 
Descriptive Properties
ColorClear
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Styroclear GH 62 SBC
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
INEOS Styrolution Styrolux® BX6400 SBC
Overview of materials for Styrene-Butadiene Copolymer, SBC
BASF Piperazine 68%

PBASF9025 / 84789

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.