MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Lupolen UHM 301 MDPE, Ultra-High Molecular Weight  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Ultra High Molecular Weight

Material Notes: For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this material contains no other additives.

Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.929 g/cc
Water Absorption 0.10 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 20.0 MPa
Elongation at Break >= 50 %
Elongation at Yield 14 %
Tensile Modulus 0.725 GPa
Tensile Creep Modulus, 1 hour 260 MPa
Tensile Creep Modulus, 1000 hours 200 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 ohm-cm
Surface Resistance 1.00e+14 ohm
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 210 µm/m-°C
@Temperature 20.0 °C
Melting Point 136 °C
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 41.0 °C
Vicat Softening Point 81.0 °C
Flammability, UL94 HB
@Thickness 0.400 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Lupolen UHM 201 MDPE, Ultra-High Molecular Weight
ExxonMobil Escorene® Escomer® H-101 Low MW HDPE Wax
Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene
Braskem HD3000N HDPE Cast Film Extrusion Polyethylene Homopolymer
Baystar™ 6410 HDPE Film Resin

PSF078 / 66655

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.