MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Escorene® Escomer® H-101 Low MW HDPE Wax  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Data provided by the manufacturer, Exxon Chemical.

A low molecular weight synthetic polyethylene wax with a unique combination of high drop point and extreme hardness coupled with an exceptionally low melt viscosity.

Applications: Hot melt adhesives; Rubber processing aid; Pigment dispersion; Candles.

Key Words: High Density Polyethylene; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³Exxon Method
Viscosity 27 cP
@Temperature 121 °C
27 cP
@Temperature 250 °F
melt viscosity; ASTM D-3236
 
Thermal PropertiesMetricEnglishComments
Melting Point 111 °C232 °FExxon Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema EVATANE® 18-150 Copolymer Ethylene - Vinyl Acetate
ExxonMobil ESCOREZ™ 5320 Petroleum Hydrocarbon Resin
ExxonMobil ESCOREZ™ 5600 Petroleum Hydrocarbon Resin
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
Baystar™ 6410 HDPE Film Resin

PEXCHS / 38012

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.