MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Telcar® TL-355 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Telcar TL-355 is a general purpose thermoplastic elastomer designed for consumer/industrial applications. Telcar TL-355 is a low density, high hardness grade suitable for both injection molding and extrusion.

Features: Filled; High Hardness; Low Density; Medium Flow; Medium Slip

Uses: Blow Molding Applications; General Purpose; Grommets; Rubber Replacement

Form: Pellets

Processing Method: Injection Molding; Extrusion

Injection Notes: Injection Rate: Moderate-Fast

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccASTM D792
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 42
@Time 5.00 sec
Injection Molded; ASTM D2240
 44
@Time 1.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 14.0 MPaFlow, Die C, 20 in/min; ASTM D412
 1760 psiAcross Flow, Die C, 20 in/min; ASTM D412
Tensile Stress at Strain 1750 psi
@Strain 100 %
Across Flow, Die C, 20 in/min; ASTM D412
 1990 psi
@Strain 100 %
Flow, Die C, 20 in/min; ASTM D412
Elongation at Break 180 %Across Flow, Die C, 20 in/min; ASTM D412
 220 %Flow, Die C, 20 in/min; ASTM D412
Tear Strength 452 pliAcross Flow, Die C, 20 in/min; ASTM D624
 515 pliFlow, Die C, 20 in/min; ASTM D624
Compression Set 41 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ASTM D395B
 79 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ASTM D395B
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 340 - 380 °F
Middle Barrel Temperature 350 - 390 °F
Front Barrel Temperature 360 - 400 °F
Nozzle Temperature 370 - 410 °F
Zone 1 330 - 370 °F
Zone 2 340 - 380 °F
Zone 3 350 - 390 °F
Zone 5 360 - 400 °F
Die Temperature 374 - 410 °F
Melt Temperature 370 - 410 °FProcessing Temperature
Mold Temperature 77.0 - 150 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Telcar® TL-340-S Thermoplastic Elastomer
Overview of materials for Epoxy Adhesive
Network Polymers Softflex® 0921
Lubrizol ESTANE® 58284 Ether Based Thermoplastic Polyurethane

PTEKNP496 / 129577

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.