MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol ESTANE® 58284 Ether Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: Matte finish, superior durability

Uses: Extrusion – wire and cable, General application

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 82 - 88
@Time 5.00 sec
82 - 88
@Time 0.00139 hour
ASTM D2240
Tensile Strength 48.3 MPa7010 psiASTM D412
Elongation at Break 550 %550 %ASTM D412/D638
100% Modulus 7.00 MPa
@Strain 100 %
1020 psi
@Strain 100 %
ASTM D412
300% Modulus 13.1 MPa
@Strain 300 %
1900 psi
@Strain 300 %
ASTM D412
Tear Strength 12.4 kN/m71.0 pliTrouser; ASTM D470
Graves Tear Strength 167 kN/m950 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 8383H-18, 1000g; ASTM D3389 B
Compression Set  19 %
@Temperature 23.0 °C,
Time 79200 sec
19 %
@Temperature 73.4 °F,
Time 22.0 hour
 68 %
@Temperature 70.0 °C,
Time 79200 sec
68 %
@Temperature 158 °F,
Time 22.0 hour
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -44.0 °C-47.2 °F
 
Processing PropertiesMetricEnglishComments
Zone 1 174 °C345 °FExtrusion
Zone 2 179 °C354 °FExtrusion
Zone 3 185 °C365 °FExtrusion
Zone 4 191 °C376 °FExtrusion
Adapter Temperature 191 °C376 °FExtrusion
Die Temperature 179 °C354 °FZone 2, Extrusion
 185 °C365 °FZone 1, Extrusion
Drying Temperature 104 °C219 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CPT C-Flex® R70-051 Clear Biocompatible TPE
Overview of materials for Nylon 66, Unreinforced
CPT C-Flex® R70-046 Clear Biocompatible TPE
CPT C-Flex® R70-028 Opaque Biocompatible TPE
CPT C-Flex® R70-026 Opaque Biocompatible TPE

PNOVEON045 / 55312

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.