MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

The NanoSteel® Company SHS 9172 TWAS Steel Alloy, Cored Wire
Categories: Metal; Ferrous Metal; Alloy Steel; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Coating Description: SHS 9172 TWAS is an iron based steel alloy with a nanoscale microstructure that features exceptional wear, corrosion and high temperature oxidation resistance in severe abrasion and fine particle erosion environments.

    Key Performance Characteristics
  • Excels in extreme environments where severe abrasion is encountered
  • Significant ability to withstand corrosion and high temperature oxidation
  • Exceptional wear resistance in applications involving fine particle abrasion and erosion
  • Superior bond strength and toughness

Application Process: Twin Wire Arc Spraying (TWAS)

Information Provided by The NanoSteel Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.68 g/cc0.277 lb/in³Coating Property
Porosity <= 5.0 %<= 5.0 %Coating Property
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 975 - 1025975 - 1025kg/mm2; HV300
Adhesive Bond Strength 41.4 - 55.2 MPa
@Thickness 0.508 mm
6000 - 8000 psi
@Thickness 0.0200 in
1018 steel; ASTM C633-01
 
Component Elements PropertiesMetricEnglishComments
Boron, B <= 5.0 %<= 5.0 %
Carbon, C <= 4.0 %<= 4.0 %
Chromium, Cr <= 25 %<= 25 %
Iron, Fe >= 38 %>= 38 %
Manganese, Mn <= 3.0 %<= 3.0 %
Molybdenum, Mo <= 6.0 %<= 6.0 %
Niobium, Nb (Columbium, Cb) <= 12 %<= 12 %
Silicon, Si <= 2.0 %<= 2.0 %
Tungsten, W <= 15 %<= 15 %
 
Descriptive Properties
Deposition Efficiency (%)80Coating Property
Impact ResistanceNo delamination/cracking at 480 in-lbsDrop Impact Testing
Wear Resistance Mass Loss (g)0.172000 cycles; ASTM G65-04 Procedure B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
HP Alloys Alloy 718, 0% Cold Worked, Not Aged
MetalTek RENE® 220 Centri-Vac Nickel Cobalt Based Alloy
Universal Wire Works ER240 Stainless Steel Bare Wire
AISI 302Cu Stainless Steel soft tempered 2.54- 25.4 mm diameter wire
446 Stainless Steel, Soft Tempered Wire

NNANO009 / 106804

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.