MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Universal Wire Works ER240 Stainless Steel Bare Wire
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: This alloy is most often used for welding UNS S24000 and UNS S24100 base metals. These alloys are nitrogen strengthened austenitic stainless steels exhibiting high strength and good toughness in a wide range of temperatures. Significant improvement of wear resistance in particle-to-metal and metal-to-metal (galling) application is a valuable characteristic when compared with more conventional austenitic stainless steels like type 304. Nitrogen alloying reduces the tendency toward intergranular carbide precipitation in the weld area and improves resistance to transgranular stress corrosion in hot aqueous chloride-containing media.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 18 %18 %
Iron, Fe 64.85 %64.85 %As Remainder
Manganese, Mn 12 %12 %
Nickel, Ni 5.0 %5.0 %
Nitrogen, N 0.15 %0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
304 Stainless Steel (UNS S30400); Cold Finished Wire
AISI Type S24100 Stainless Steel 6.4 mm diameter annealed rod, 0% cold reduction
AISI Type 316L Stainless Steel, annealed bar
AISI Type 316LN Stainless Steel, Composition Spec
316 Stainless Steel, annealed plate

NUWW042 / 19607

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.