MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Monprene® SP-16920 XRD2 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene SP-16920 XRD2 is a general purpose thermoplastic elastomer designed for a variety of consumer applications, requiring a soft, rubber-like feel. Monprene SP-16920 XRD2 is a low hardness, low density grade that exhibits a good toughness and is suitable for injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Colorability; Good Flexibility; Good Moldability; Good Toughness; Low Density; High Elongation; Resilient; Soft

Uses: Rubber Replacement; Sporting Goods; Swimming Pools; Water Sports Equipment

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.882 g/cc0.0319 lb/in³ASTM D792
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
15 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  19
@Time 5.00 sec
19
@Time 0.00139 hour
Injection Molded; ASTM D2240
 20
@Time 1.00 sec
20
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 1.81 MPa263 psiASTM D412
Elongation at Break >= 600 %>= 600 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 182 - 232 °C360 - 450 °F
Middle Barrel Temperature 188 - 238 °C370 - 460 °F
Front Barrel Temperature 193 - 243 °C380 - 470 °F
Nozzle Temperature 199 - 249 °C390 - 480 °F
Melt Temperature 199 - 249 °C390 - 480 °F
Mold Temperature 35.0 - 48.9 °C95.0 - 120 °F
Injection Pressure 1.38 - 5.52 MPa200 - 800 psi
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceNatural Color
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Monprene® SP-14966 Thermoplastic Elastomer
Teknor Apex Monprene® SP-14986 XRD1 Thermoplastic Elastomer
Teknor Apex Monprene® SP-14077 Thermoplastic Elastomer
Lanxess Mesamoll® Plastic Additive
Lanxess Mesamoll® II Plastic Additive

PTEKNQ0961 / 237452

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.