MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Mesamoll® II Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Mesamoll® II is a phthalate-free general purpose plasticizer with a good gelling behavior and an exceptional saponification resistance. It is compatible with many types of polymers including PVC, polyurethanes, and rubber. The main difference between Mesamoll® II and Mesamoll® is the former’s reduced volatility.

Chemical composition: alkylsulfonic acid ester with phenol (ASE)

CAS Reg. No: 91082-17-6 (ASE)

General

  • a lower volatility than Mesamoll®
  • a good compatibility with a large number of polymers
  • an excellent gelling capacity with a large number of polymers including PVC, resulting in lower processing temperatures and shorter processing times.
  • a good resistance to weathering.
  • a high saponification resistance due to Mesamoll®'s chemical structure (Fig. 3). This is especially beneficial for articles which come into contact with water and alkalis.
  • favorable dielectric properties for high frequency welding, leading to short cycle times.
Applications: Mesamoll® II is used as a plasticizer for a wide range of articles based on polyvinyl chloride (PVC), polyurethane (PUR), and rubbers (NBR, NR, SBR, SBR/BR, IIR, CR). Mesamoll® II allows the production of AgBB conform articles. Typical applications are:
  • Polyurethane-based sealing and adhesive systems (One-component and two component systems) Moldable, easy-to-process sealants for filling or covering joints in structures and parts of buildings.
  • Cleaning: Rinsing and service fluids for polyurethane foaming machinery.
  • Rotational Molding: Vinyl articles made by rotational casting.
  • Dip Molding: PVC one way gloves and other articles which are produced by dip molding.
  • Calendering: Film for the automotive industry, film for tunnel linings and other construction applications, swimming pool covers, shower curtains, office film, welding film, film for electrical insulation, adhesive tape.
  • Extrusion: Profiles for the automotive industry, jointing strip, tubing, weathering and alkali-resistant structural profiles, blown film.
  • Injection Molding: Work boots, technical articles.
  • Coatings (including spreading): Coatings for air-supported structures and tents, occupational and protective clothing, rain-wear, bath mats, expanded film, floor coverings, wall paper, imitation leather.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.03 g/cc
@Temperature 57.0 °C
0.0372 lb/in³
@Temperature 135 °F
DIN 51 757
 1.04 g/cc
@Temperature 42.0 °C
0.0376 lb/in³
@Temperature 108 °F
DIN 51 757
 1.05 g/cc
@Temperature 29.0 °C
0.0379 lb/in³
@Temperature 84.2 °F
DIN 51 757
 1.055 g/cc
@Temperature 20.0 °C
0.03811 lb/in³
@Temperature 68.0 °F
DIN 51 757
Volatiles <= 0.25 %<= 0.25 %paraffinic components; K27001/MEL
Water Absorption <= 0.050 %<= 0.050 %DIN 51 777
Viscosity 135 cP135 cPDIN 53 015
 20 cP
@Temperature 60.0 °C
20 cP
@Temperature 140 °F
DIN 53 015
 40 cP
@Temperature 44.0 °C
40 cP
@Temperature 111 °F
DIN 53 015
 60 cP
@Temperature 35.0 °C
60 cP
@Temperature 95.0 °F
DIN 53 015
 80 cP
@Temperature 29.0 °C
80 cP
@Temperature 84.2 °F
DIN 53 015
 100 cP
@Temperature 25.0 °C
100 cP
@Temperature 77.0 °F
DIN 53 015
 120 cP
@Temperature 23.0 °C
120 cP
@Temperature 73.4 °F
DIN 53 015
 
Thermal PropertiesMetricEnglishComments
Pour Point -35.6 °C-32.0 °FISO 3016
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.501.50DIN EN ISO 6320
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Color<300Hazen, DIN ISO 6271
Specifications120°CDissolution temp, DIN 53 408

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Monprene® SP-14966 Thermoplastic Elastomer
Geon® Performance Solutions 130 Series 138 Polyvinyl Chloride Copolymer (PVC Copolymer)
Geon® Performance Solutions 120 Series 129 Polyvinyl Chloride Homopolymer
Geon® Performance Solutions 120 Series 120X400 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Lanxess Mesamoll® Plastic Additive

PLANY8904 / 209296

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.