MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions 120 Series 120X400 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Geon® 120X400 is medium molecular weight resin providing a good balance of fusion temperatures and film physical properties. It gives good chemical foamability for producing medium to high density foams. It contains lower emulsifier level results in lower plate-out without the loss of foamability as compared to standard Geon® 120A resin. Geon® 120X400 is recommended for medium to high density foam or solid applications where good fused film physical properties are required such as stand coating, resilient flooring foam layer, artificial leather and suede type fabrics.

Note: The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Geon® ALTC and ASTM D638 (formulation): 100phr Geon® 120X400, 57phr DINP, 3phr ESO, and 2phr Therm-Chek SP 120 LOHF Geon® STP 390(formulation): 100phr Geon® 120X400, and 60phr DOP

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Bulk Density 0.465 g/cc0.0168 lb/in³
Fineness 4.754.75Hegman, North Fineness; Geon® 390
Relative Viscosity 2.37 cP2.37 cPCorrelation, Cyclohexanone 1%; Internal Method
Brookfield Viscosity 4.88 cP4.88 cPInitial Viscosity @ 20 rpm; Geon® ALTC 22 (with provided formulation); Internal Method
 5.5 cP5.5 cPInitial Viscosity @ 2 rpm; Geon® ALTC 22 (with provided formulation); Internal Method
 6.1 cP6.1 cPOne Day Viscosity @ 20 rpm; Geon® ALTC 22 (with provided formulation); Internal Method
 6.98 cP6.98 cPOne Day Viscosity @ 2 rpm; Geon® ALTC 22 (with provided formulation); Internal Method
Viscosity Measurement 1.01.0Inherent; ASTM D1243-60-A
Melt Flow 102 g/10 min
@Pressure 0.655 MPa
102 g/10 min
@Pressure 95.0 psi
Severs Efflux; Geon® ALTC 23 (with provided formulation); Internal Method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 21.0 MPa3050 psiOptimum; With provided formulation; ASTM D638
 
Optical PropertiesMetricEnglishComments
Gloss 82 %82 %60 Degree Fused 5 mins @ 350 F Geon® ALTC 65 (with provided formulation); Internal Method
Transmission, Visible 81 %81 %Geon® ALTC 66 (with provided formulation); Internal Method
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.050 %0.050 %Karl FisherGeon® STP 683; Internal Method
 
Descriptive Properties
FeaturesFoamable
 Medium Molecular Weight
FormsPowderFine, WHite Powder
Gel Temperature71 °CInternal Method; Geon® ALTC 29 (with provided formulation)
Generic MaterialPVC Homopolymer
Generic NamePolyvinyl Chloride Homopolymer (PVC Homopolymer)
K-Value70Internal Method; Correlation, (0.5gm/100ml)
Methanol Extractables2.9%Internal Method; Geon® STP 894
Polymerization ProcessMicrosuspension
Processing MethodCoating
 Dip Coating
 Rotational Molding
 Slush Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Residual Vinyl Chloride Monomer< 9 ppmInternal Method; Geon® STP 1005
UsesCoating Applications
 Film
 Foam
 Textile Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions FIT E 50 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Performance Solutions 120 Series 129 Polyvinyl Chloride Homopolymer
Geon® Performance Solutions 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer)
Geon® Performance Solutions 130 Series 138 Polyvinyl Chloride Copolymer (PVC Copolymer)
Overview of materials for PVC, 20% Glass Fiber Reinforced

PH0POL0857 / 145426

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.