MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tra-Con Tra-Bond 2212 High Temperature Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, High Temperature

Material Notes: TRA-BOND 2212 was developed for high temperature bonding, laminating, filament winding and potting applications where the combination of good physical and mechanical properties plus superior wetting and handling characteristics is required. This dark amber, all liquid formulation contains no solvents, and is easily mixed, handled and applied at room temperature, however a final elevated-temperature cure step is required for complete cure. TRA-BOND 2212 develops strong, tough bonds to metals, glass and glass fabrics, ceramics and many other electronic an aerospace materials. The fully cured adhesive exhibits low weight loss and an improved retention of mechanical properties at elevated service temperatures. It also displays excellent chemical resistance and low permeability to gases and vapors coupled with superior electrical insulation properties. In addition, TRA-BOND 2212 provides very good resistance to water, weather, jet fuels, most petroleum products, salt solutions, mild acids and alkalis, and many other organic and inorganic compounds. For masses over 1/4 gram, step cure the material for 2 hours @ 75°C, followed by 1 hour @ 150°C. This step cure schedule can also be used for low stress applications.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccMixed
Viscosity 21500 cP
@Temperature 25.0 °C
21500 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8989
Tensile Strength, Yield 47.6 MPa6900 psi
Elongation at Yield 2.0 %2.0 %
Adhesive Bond Strength 16.5 MPa2400 psiLap shear, adhesion to glass
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.70e+14 ohm-cm7.70e+14 ohm-cm
Dielectric Constant 3.9
@Frequency 1000 Hz
3.9
@Frequency 1000 Hz
Dielectric Strength 15.6 kV/mm395 kV/in
Dissipation Factor 0.010
@Frequency 1000 Hz
0.010
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear  71.0 µm/m-°C
@Temperature 20.0 °C
39.4 µin/in-°F
@Temperature 68.0 °F
Alpha 1
 171 µm/m-°C
@Temperature 20.0 °C
95.0 µin/in-°F
@Temperature 68.0 °F
Alpha 2
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 155 °C311 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 150 °C
1.00 hour
@Temperature 302 °F
Pot Life 1440 min1440 min(1 day)
 
Descriptive Properties
Color Dark Amber
Heat Distortion Temperature °C158
Mix Ratio, parts by weight100/3Resin/Hardener
Thixotropic Index 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 2211 High Temperature Epoxy Adhesive
Epoxy Technology EPO-TEK® 383ND High Temperature Epoxy
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy
Epoxy Technology EPO-TEK® 375 High Temperature Epoxy
Epoxy Technology EPO-TEK® 360T High Temperature Epoxy

PTRAC061 / 70989

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.