MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epoxy Technology EPO-TEK® 383ND High Temperature Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, High Temperature

Material Notes: Material Description: A slightly longer pot life version of EPO-TEK®353ND designed for high temperature, optical and structural applications inside the semiconductor, hybrid, electronic, fiber optic and medical industries.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/ccPart B
 1.20 g/cc1.20 g/ccPart A
Particle Size <= 20 µm<= 20 µm
Viscosity 3500 - 6000 cP
@Temperature 23.0 °C
3500 - 6000 cP
@Temperature 73.4 °F
50 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888
Tensile Modulus 2.54 GPa369 ksiStorage
Shear Strength >= 13.8 MPa>= 2000 psiLap
 >= 46.9 MPa>= 6800 psiDie
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 3.00e+13 ohm-cm>= 3.00e+13 ohm-cm
Dielectric Constant 2.58
@Frequency 1000 Hz
2.58
@Frequency 1000 Hz
Dissipation Factor 0.0080
@Frequency 1000 Hz
0.0080
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 34.0 µm/m-°C18.9 µin/in-°FBelow Tg
 129 µm/m-°C71.7 µin/in-°FAbove Tg
Maximum Service Temperature, Air 250 °C482 °FContinuous
 350 °C662 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg >= 100 °C>= 212 °FDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 415 °C779 °FDegradation Temperature
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5715
@Wavelength 589 nm
1.5715
@Wavelength 589 nm
Transmission, Visible >= 90 %
@Wavelength 520 - 1660 nm
>= 90 %
@Wavelength 520 - 1660 nm
Spectral
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min
@Temperature 90.0 °C
0.500 hour
@Temperature 194 °F
minimum
Pot Life 480 min480 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
 
Descriptive Properties
ColorClearPart A
 Slightly YellowPart B
ConsistencyPourable liquid
Mix Ratio by Weight10:1
Number of ComponentsTwo
Weight Loss0.28%200°C
 0.42%250°C
 0.86%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 353ND High Temperature Epoxy
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy
Epoxy Technology EPO-TEK® 375 High Temperature Epoxy
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy
Epoxy Technology EPO-TEK® OE100-T High Temperature Epoxy

PPOXYT133 / 141172

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.