MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ DP810 Black Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel strength along with good impact resistance and durability. They can quickly bond to most metals, ceramics, rubbers, plastics and wood with minimal surface preparation.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 17000 - 21000 cPAccelerator
 18000 - 22000 cPBase
 20000 cP
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 30.0 psiOverlap at 10 minutes after bonding
 50.0 psiOverlap, Acetone for 14 days, Cohesive Failure
 75.0 psiOverlap, MEK for 14 days, Cohesive Failure
 500 psiOverlap, Polycarbonate, Adhesive/Cohesive Failure
 550 psiOverlap, Acrylic, Substrate Failure
 700 psiOverlap, ABS, Adhesive/Cohesive Failure
 1000 psiOverlap, PVC, Substrate Failure
 1150 psiOverlap at 20 minutes after bonding
 1500 psiOverlap, 71°C 100% RH for 14 days, Mixed Mode of AF&CF
 1650 psiOverlap, 71°C soak for 14 days, Mixed Mode of AF&CF
 2200 psiOverlap at 1 hr after bonding
 2550 psiOverlap, Gasoline for 14 days, Cohesive Failure
 2600 psiOverlap, Toluene for 14 days, Cohesive Failure
 2700 psiOverlap at 2 hrs after bonding
 2900 psiOverlap at 2 hrs after bonding
 3000 psiOverlap, Green FRP, Cohesive Failure
 3050 psiOverlap, IPA for 14 days, Cohesive Failure
 3200 psiOverlap at 2 hrs after bonding
 3250 psiOverlap, 20% Bleach for 14 days, Cohesive Failure
 3450 psiOverlap, Oily CRS, Cohesive Failure
 3500 psiOverlap, Stainless Steel, Cohesive Failure
 3550 psiOverlap at 2 hrs after bonding
 3600 psiOverlap, CRS, Cohesive Failure
 3750 psiOverlap, Abraded Aluminum, Cohesive Failure
 3750 psiOverlap, 14 days, Cohesive Failure
 3850 psiOverlap, Bare Aluminum, Cohesive Failure
 3900 psiOverlap, 50% Antifreeze for 14 days, Cohesive Failure
 3950 psiOverlap, Diesel Fuel for 14 days, Cohesive Failure
 4200 psiOverlap, Etched Aluminum, Cohesive Failure
 500 psi
@Temperature 82.0 °C
Overlap
 1200 psi
@Temperature -55.0 °C
Overlap
 2000 psi
@Temperature -29.0 °C
Overlap, Adhesion Failure
 2000 psi
@Temperature 49.0 °C
Overlap, Cohesive Failure
 3600 psi
@Temperature 24.0 °C
Overlap
Peel Strength 30.0 pliT-Peel
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 - 20.0 minTime to Handling Strength
 8.00 - 24.0 hourFull cure
 
Descriptive Properties
AppearanceBlackBase
 WhiteAccelerator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ITW Devcon Metal Welder™ Methacrylate Adhesive, Grey / Beads
ExxonMobil LDPE LD 615BA Low Density Polyethylene Resin (European Grade)
3M Scotch-Weld™ DP810 Tan Structural Adhesive
3M Scotch-Weld™ DP640 Structural Adhesive
3M Scotch-Weld™ DP-605NS Off-White Adhesive in Duo-Pak Cartridges

PMM34666 / 169413

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.