MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M Scotch-Weld™ DP810 Tan Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel strength along with good impact resistance and durability. They can quickly bond to most metals, ceramics, rubbers, plastics and wood with minimal surface preparation.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 18000 - 22000 cP18000 - 22000 cPAccelerator
 18000 - 22000 cP18000 - 22000 cPBase
 20000 cP20000 cP
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 0.345 MPa50.0 psiOverlap, MEK for 14 days, Cohesive Failure
 0.345 MPa50.0 psiOverlap at 10 minutes after bonding
 0.517 MPa75.0 psiOverlap, Acetone for 14 days, Cohesive Failure
 2.76 MPa400 psiOverlap, Diesel Fuel for 14 days, Cohesive Failure
 4.14 MPa600 psiOverlap, ABS, Adhesive/Cohesive Failure
 5.86 MPa850 psiOverlap, Polycarbonate, Adhesive/Cohesive Failure
 6.89 MPa1000 psiOverlap, PVC, Substrate Failure
 7.58 MPa1100 psiOverlap, Acrylic, Substrate Failure
 10.3 MPa1500 psiOverlap, 71°C 100% RH for 14 days, Mixed Mode of AF&CF
 10.3 MPa1500 psiOverlap at 20 minutes after bonding
 12.1 MPa1750 psiOverlap, 71°C soak for 14 days, Mixed Mode of AF&CF
 15.5 MPa2250 psiOverlap at 1 hr after bonding
 17.6 MPa2550 psiOverlap, Gasoline for 14 days, Cohesive Failure
 17.9 MPa2600 psiOverlap at 2 hrs after bonding
 18.3 MPa2650 psiOverlap, Toluene for 14 days, Cohesive Failure
 19.0 MPa2750 psiOverlap at 2 hrs after bonding
 20.3 MPa2950 psiOverlap at 2 hrs after bonding
 21.4 MPa3100 psiOverlap, CRS, Cohesive Failure
 21.7 MPa3150 psiOverlap, IPA for 14 days, Cohesive Failure
 23.1 MPa3350 psiOverlap at 2 hrs after bonding
 23.4 MPa3400 psiOverlap, Stainless Steel, Cohesive Failure
 23.8 MPa3450 psiOverlap, Oily CRS, Cohesive Failure
 23.8 MPa3450 psiOverlap, 20% Bleach for 14 days, Cohesive Failure
 25.9 MPa3750 psiOverlap, 14 days, Cohesive Failure
 26.2 MPa3800 psiOverlap, Bare Aluminum, Cohesive Failure
 26.2 MPa3800 psiOverlap, Green FRP, Cohesive Failure
 26.5 MPa3850 psiOverlap, 50% Antifreeze for 14 days, Cohesive Failure
 26.9 MPa3900 psiOverlap, Abraded Aluminum, Cohesive Failure
 29.0 MPa4200 psiOverlap, Etched Aluminum, Cohesive Failure
 3.45 MPa
@Temperature 82.0 °C
500 psi
@Temperature 180 °F
Overlap
 8.27 MPa
@Temperature -55.0 °C
1200 psi
@Temperature -67.0 °F
Overlap
 12.1 MPa
@Temperature -29.0 °C
1750 psi
@Temperature -20.2 °F
Overlap, Adhesion Failure
 13.8 MPa
@Temperature 49.0 °C
2000 psi
@Temperature 120 °F
Overlap, Cohesive Failure
 24.8 MPa
@Temperature 24.0 °C
3600 psi
@Temperature 75.2 °F
Overlap
Peel Strength 5.26 kN/m30.0 pliT-Peel
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 - 20.0 min0.167 - 0.333 hourTime to Handling Strength
 480 - 1440 min8.00 - 24.0 hourFull cure
 
Descriptive Properties
AppearanceGreenBase
 WhiteAccelerator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LDPE LD 615BA Low Density Polyethylene Resin (European Grade)
3M Scotch-Weld™ DP810 Black Structural Adhesive
3M Scotch-Weld™ DP640 Structural Adhesive
3M Scotch-Weld™ DP-605NS Off-White Adhesive in Duo-Pak Cartridges
3M Scotch-Weld™ DP420 Black Epoxy Adhesive

PMM34665 / 169412

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.