Product Description: LD 615BA is a medium flow LDPE grade, characterized by high stiffness and good toughness. Availability: Africa & Middle East and Europe Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: No
Applications: - Caps
- Closures
- Compounding
- Food Packaging Containers
- Houseware Articles
- Injection Molding
- Masterbatch Base Resin
- Technical Parts
Information provided by ExxonMobil |