Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of lamination films. Availability: Africa & Middle East and Europe Additive: - Antiblock: 1800 ppm
- Slip: 330 ppm
- Thermal Stabilizer: Yes
Applications: - Co-Extrusion Films
- Display Packaging Film
- Food packaging
- Form Fill and Seal Packaging
- High Quality Lamination
- Lamination Film
Information provided by ExxonMobil |