MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Pearlthane® MB-9010 Thermoplastic Polyurethane Elastomer
Categories: Ceramic; Oxide; Titanium Oxide; Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Pearlthane® MB-9010 is a TPU-based color masterbatch, supplied in the form of homogenously white-colored pellets. It is specially intended for coloring TPUs (either polyester or polyether-based), for extrusion, injection molding or calendering processes.

Applications:

Pearlthane MB-9010 can be mixed with any items of Merquinsa's Pearlthane or Pearlcoat lines (either polyester or polyether-based) intended for applications obtained by extrusion, injection molding or calendering.

A 2% usage level (on TPU, by weight) is recommended. Higher levels can be considered, depending on the requirements of the end-product. A good color consistency requires an accurate dosing and good distribution in the TPU.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Apparent Bulk Density 1.05 g/ccASTM D-1875
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 240 °C
Drying Temperature 100 - 110 °C
@Time 3600 - 7200 sec
In hot air circulatory, vacuum, or desiccant-air dryer
 
Component Elements PropertiesOriginal ValueComments
TiO2 60 %
 
Descriptive Properties
Color Index n0RAL 9010
Lightfastness8(1-8) Scale of blue tones; DIN 53 389

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® MB-51UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Evonik TEGOMER® FR 100 Additive
Lubrizol Advanced Materials PEARLTHANE® 11T85UV Thermoplastic Polyurethane Elastomer

PMEQU962 / 109199

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.