MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ferralium Alloy 255 solution heat treated, hardened at 510°C (950°F) for 4 hours
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel

Material Notes: Patented, ferritic-austenitic; high mechanical strength, ductility, and hardness with resistance to corrosion and erosion. Excellent resistance to acids and salts. Duplex alloy with nearly equal portions of austenite and ferrite-matrix phases. Applications include pumps, agitators, valves, and piping for handling wet phosphoric acid slurries, marine scrubbers, pumps and seals, and acid handling equipment.

Key Words: UNS S32550
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.81 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 304
@Diameter 12.7 mm
Converted from Rockwell C hardness.
 326
@Diameter 6.35 mm
Converted from Rockwell C hardness.
Hardness, Knoop 326
@Diameter 12.7 mm
Converted from Rockwell C hardness.
 352
@Diameter 6.35 mm
Converted from Rockwell C hardness.
Hardness, Rockwell C 32
@Diameter 12.7 mm
 35
@Diameter 6.35 mm
Hardness, Vickers 316
@Diameter 12.7 mm
Converted from Rockwell C hardness.
 340
@Diameter 6.35 mm
Converted from Rockwell C hardness.
Tensile Strength, Ultimate 855 MPa
@Diameter 6.35 mm
 876 MPa
@Diameter 12.7 mm
 883 MPa
@Diameter 9.52 mm
 903 MPa
@Diameter 3.17 mm
 910 MPa
@Diameter 4.762 mm
 938 MPa
@Diameter 19.0 - 25.4 mm
 979 MPa
@Diameter 0.838 - 2.10 mm
Tensile Strength, Yield 641 MPa
@Strain 0.2 %,
Diameter 12.7 mm
 683 MPa
@Strain 0.2 %,
Diameter 6.35 mm
 683 MPa
@Strain 0.2 %,
Diameter 9.52 mm
 689 MPa
@Diameter 4.762 mm,
Strain 0.2 %
 703 MPa
@Diameter 3.17 mm,
Strain 0.2 %
 717 MPa
@Diameter 19.0 - 25.4 mm,
Strain 0.2 %
 772 MPa
@Diameter 0.838 - 2.10 mm,
Strain 0.2 %
Elongation at Break 22 %
@Diameter 0.838 - 2.10 mm
in 50 mm
 24 %
@Diameter 3.17 mm
in 50 mm
 24 %
@Diameter 4.762 mm
in 50 mm
 26 %
@Diameter 6.35 mm
in 50 mm
 28 %
@Diameter 19.0 - 25.4 mm
in 50 mm
 30 %
@Diameter 9.52 mm
in 50 mm
 31 %
@Diameter 12.7 mm
in 50 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000840 ohm-cm
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µm/m-°C
@Temperature 20.0 - 93.0 °C
 11.7 µm/m-°C
@Temperature 20.0 - 205 °C
 12.1 µm/m-°C
@Temperature 20.0 - 315 °C
 12.4 µm/m-°C
@Temperature 20.0 - 425 °C
 13.0 µm/m-°C
@Temperature 20.0 - 540 °C
Specific Heat Capacity 0.480 J/g-°CTypical value for stainless steel.
Thermal Conductivity 15.1 W/m-K
@Temperature 100 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.040 %
Chromium, Cr 26 %
Copper, Cu 1.7 %
Iron, Fe 62 %
Manganese, Mn 0.80 %
Molybdenum, Mo 3.3 %
Nickel, Ni 5.5 %
Nitrogen, N 0.17 %
Silicon, Si 0.45 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ferralium Alloy 255 solution treated at 1120°C, cooled rapidly
ATI Allegheny Ludlum Alloy 255 Duplex Stainless Steel, UNS S32550
Sandvik SAF 2507 Plate, Sheet and Coil
AK Steel 2205 Duplex Stainless steel
Ferralium Alloy 255 heat treated at 1120°C, cooled rapidly, 10.2-19 mm thick plate

MQN255H / 13875

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.