MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allegheny Ludlum Alloy 255 Duplex Stainless Steel, UNS S32550
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Alloy 255 is a 25% chromium duplex ferritic-austenitic stainless steel designed to provide a superior combination of high strength and excellent corrosion resistance for a wide variety of applications. The alloy possesses a microstructure which is a balanced mixture of austenite and ferrite. The combination of these phases develops the unique combination of strength and chloride stress-corrosion cracking resistance of this alloy. The alloy finds applications in marine corrosion areas, equipment for phosphoric acid and fertilizer industry, pollutions control equipment, the pulp and paper industry and the petrochemical industry.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.728 g/cc0.2792 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 302<= 302
Hardness, Rockwell C <= 32<= 32
Tensile Strength, Ultimate >= 758 MPa>= 110000 psi
Tensile Strength, Yield >= 552 MPa
@Strain 0.2 %
>= 80100 psi
@Strain 0.2 %
Elongation at Break >= 15 %>= 15 %in 2"
Charpy Impact 191 - 212 J141 - 156 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000821 ohm-cm0.0000821 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.1 µm/m-°C
@Temperature 20.0 - 100 °C
6.72 µin/in-°F
@Temperature 68.0 - 212 °F
 12.9 µm/m-°C
@Temperature 23.0 - 250 °C
7.17 µin/in-°F
@Temperature 73.4 - 482 °F
 13.8 µm/m-°C
@Temperature 23.0 - 500 °C
7.67 µin/in-°F
@Temperature 73.4 - 932 °F
Specific Heat Capacity 0.481 J/g-°C
@Temperature 52.0 °C
0.115 BTU/lb-°F
@Temperature 126 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.0400 %<= 0.0400 %
Chromium, Cr 24 - 27 %24 - 27 %
Copper, Cu 1.5 - 2.5 %1.5 - 2.5 %
Iron, Fe 60 - 67 %60 - 67 %as balance
Manganese, Mn <= 1.50 %<= 1.50 %
Molybdenum, Mo 2.9 - 3.9 %2.9 - 3.9 %
Nickel, Ni 4.5 - 6.5 %4.5 - 6.5 %
Nitrogen, N 0.10 - 0.25 %0.10 - 0.25 %
Phosphorus, P <= 0.0400 %<= 0.0400 %
Silicon, Si <= 1.00 %<= 1.00 %
Sulfur, S <= 0.0300 %<= 0.0300 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ferralium Alloy 255 solution treated at 1120°C, cooled rapidly
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Ferralium Alloy 255 solution heat treated, hardened at 510°C (950°F) for 4 hours
AISI Type 316L Stainless Steel, annealed plate
Outokumpu 2205 Duplex Stainless Steel

NL255 / 17831

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.