MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Fibre Glast 77 Wax-Free General Purpose Polyester Molding Resin
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: Description:#77 Molding Resin is ideal for general purpose part fabrication and for building low cost molds. An internal thickening agent has been added to prevent drainage on vertical surfaces, yet it retains the low viscosity required for rapid wet out. This resin is wax free to reduce sanding between coats. #77 Polyester Molding Resin is a prepromoted, thixotropic, general purpose resin.

Performance:
  • High thixotropic index to prevent draining on vertical surfaces
  • Low viscosity fir fast wet-out
  • Styrene suppressed

Suggested Uses:#77 Polyester Molding Resin can be used for hand lay-up or spray-up for general fiberglass reinforced plastics applications.

Information provided by Fibre Glast Developments Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 56 %
Brookfield Viscosity 475 cP#2 Spindle, 30 rpm
 
Thermal PropertiesOriginal ValueComments
Flash Point 73.0 - 100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 min
@Temperature 25.0 °C
using 1.25% #69 Catalyst
Gel Time 15.0 minAt 77°F using 1.25% #69 Catalyst
 
Descriptive Properties
Maximum Exotherm320°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® EVA-1120 Ethylene Vinyl Acetate (EVA)
A-Glass Fiber, Generic
BCC Products BC 83 Liquid Wax Painting/White
Dow 2-5088 Wax
Evonik VESTOWAX® GTL Sarawax SX 105 Crude Fischer-Tropsch Wax

PFIBRE26 / 38294

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.