MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTOWAX® GTL Sarawax SX 105 Crude Fischer-Tropsch Wax
Categories: Polymer

Material Notes: Synthetic Waxes: With its VESTOWAXR product range Evonik offers synthetic waxes produced by Fischer-Tropsch-Process. This process yields straight-chain products possessing low viscosity in the melt and having molecular weights of between 500 and 1,000 g/mol. The definition of the term ›wax‹ is based less on the chemical composition of a substance than on its physical properties:
  • kneadable at 20 °C, with a consistency ranging from solid to brittle-hard
  • coarsely to finely crystalline, translucent to opaque
  • melt above 40 °C without decomposition
  • already of relatively low viscosity at just above the melting point
  • highly temperature-dependent consistency and solubility
  • can be polished under gentle pressure
In addition to crude FT-wax, the range of VESTOWAXR products includes modified hard paraffins, oxidates and partially saponified waxes. Depending on the supply form different bags sizes are offered: Prills and micro prills usually in 25 kg bags or 700 kg big bags, pellets, flakes and coarse powder usually in 20 kg bags, microfine powder usually in 15 kg bags.

Your benefits:

  • solutions for a multitude of applications
  • extensive range of FT-modified grades
  • wide variety of supply forms- from pellets to microfine powder

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³DIN 53 479
Viscosity <= 20 cP
@Temperature 130 °C
<= 20 cP
@Temperature 266 °F
DIN 52 007/1
Molecular Weight 900 g/mol900 g/mol
 
Mechanical PropertiesMetricEnglishComments
Penetration P(0), 1/10 mm 1.01.0ASTM D1321
 
Thermal PropertiesMetricEnglishComments
Dropping Point 114 - 120 °C237 - 248 °FASTM D566
 
Descriptive Properties
AppearanceWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® EVA-1120 Ethylene Vinyl Acetate (EVA)
Fibre Glast 77 Wax-Free General Purpose Polyester Molding Resin
ExxonMobil Escorene® Escomer® H-101 Low MW HDPE Wax
Evonik VESTOWAX® P 730 Modified PP Wax
Evonik VESTOWAX® GTL Sarawax SX 100 Crude Fischer-Tropsch Wax

PEVONIL124 / 196328

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.