MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bamberger Polymers Bapolene® EVA-1120 Ethylene Vinyl Acetate (EVA)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: This resin is a general purpose resin for extrusion/injection molding applications. Parts made with this product exhibit excellent flexibility, resilience, toughness, and ESCR properties.

Applications: Compounding; Footwear; Hose; Profiles; Pump Parts; Sporting Goods; Tubing

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: Good Flexibility; Good Toughness; High ESCR (Stress Crack Resist.); Resilient
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.938 g/cc0.0339 lb/in³ASTM D1505
Vinyl Acetate Content 18 %18 %
Melt Flow 2.0 g/10 min2.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 15.17 MPa2200 psi(2.0 in/min); ASTM D638
Elongation at Break 720 %720 %(2.0 in/min); ASTM D638
Flexural Modulus, 1% Secant 59.98 MPa8700 psiASTM D790
 
Descriptive Properties
processExtrusion
 Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyamide-Imide, Molded
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled
Bamberger Polymers Bapolene® EVA-1122 Ethylene Vinyl Acetate (EVA)
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
Dow Elvax® 3178Z Ethylene Vinyl Acetate

PBP1134 / 193450

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.