MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Noble Polymers Regis™ 190108 Thermoplastic Olefin (TPO)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE; Thermoplastic Olefinic Elastomer (TPO); TPO

Material Notes: Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, material handling, step pads and other applications requiring rigid TPOs. This recyclable product is a tough, high-strength thermoplastic that maintains its properties over a wide temperature range.

Information provided by Noble Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM D955
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.01 MPa2902 psiASTM D638
Elongation at Break 185.8 %185.8 %ASTM D412
Izod Impact, Notched  4.68 J/cm
@Temperature -30.0 °C
8.77 ft-lb/in
@Temperature -22.0 °F
ASTM D256
 6.09 J/cm
@Temperature 23.0 °C
11.4 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Gardner Impact  20.3 J
@Temperature 23.0 °C
15.0 ft-lb
@Temperature 73.4 °F
ASTM D5420
 22.64 J
@Temperature -30.0 °C
16.70 ft-lb
@Temperature -22.0 °F
ASTM D5420
Tangent Modulus 1310 MPa190000 psiASTM D790
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 191 - 218 °C375 - 425 °F
Ejection Temperature 26.7 - 54.4 °C80.0 - 130 °FWater Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Termopol Termoton® K2GA3060A TPE Compound, based on SEBS and Polyolefins
Stellarchem AB835EM TPE Compound
RTP Company ESD C 2700-75A Saturated Styrenic Block Copolymer, ESD Protection - Electrically Conductive
DSM Arnitel® EM402-L Polyether Ester Elastomer (European Grade)
Barlog Plastics KEBAFLEX P D35.1 Polyester-Elastomer, Shore D35

PNOBLE17 / 54827

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.