MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Noble Polymers Regis™ 190108 Thermoplastic Olefin (TPO)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE; Thermoplastic Olefinic Elastomer (TPO); TPO

Material Notes: Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, material handling, step pads and other applications requiring rigid TPOs. This recyclable product is a tough, high-strength thermoplastic that maintains its properties over a wide temperature range.

Information provided by Noble Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Linear Mold Shrinkage 0.010 cm/cmASTM D955
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2902 psiASTM D638
Elongation at Break 185.8 %ASTM D412
Izod Impact, Notched 8.77 ft-lb/in
@Temperature -30.0 °C
ASTM D256
 11.4 ft-lb/in
@Temperature 23.0 °C
ASTM D256
Gardner Impact 180 in-lb
@Temperature 23.0 °C
ASTM D5420
 200.4 in-lb
@Temperature -30.0 °C
ASTM D5420
Tangent Modulus 190000 psiASTM D790
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 375 - 425 °F
Ejection Temperature 80.0 - 130 °FWater Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Termopol Termoton® K2GA3060A TPE Compound, based on SEBS and Polyolefins
Stellarchem AB835EM TPE Compound
RTP Company ESD C 2700-75A Saturated Styrenic Block Copolymer, ESD Protection - Electrically Conductive
DSM Arnitel® EM402-L Polyether Ester Elastomer (European Grade)
Barlog Plastics KEBAFLEX P D35.1 Polyester-Elastomer, Shore D35

PNOBLE17 / 54827

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.