MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Stellarchem AB835EM TPE Compound
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE

Material Notes: This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, completely recyclable, colorable & non-hygroscopic thermoplastics elastomer material.

Information provided by Stellarchem Polymer & Industrial

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Particle Mesh Size 80 - 150 Mesh80 - 150 Mesh
Melt Flow 12.66 g/10 min12.66 g/10 minJIS K7210
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3838JIS K6301
Tensile Strength, Ultimate 1.08 MPa156 psiJIS K6301
Elongation at Break 547 %547 %JIS K6301
100% Modulus 0.686 MPa
@Strain 100 %
99.5 psi
@Strain 100 %
JIS K6301
300% Modulus 0.588 MPa
@Strain 300 %
85.3 psi
@Strain 300 %
JIS K6301
Tear Strength 9.51 kN/m54.3 pliJIS K6301-B
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 - 220 °C392 - 428 °FMetering Temperature, Extrusion
Rear Barrel Temperature 160 - 180 °C320 - 356 °FInjection Molding
 160 - 180 °C320 - 356 °FExtrusion
Middle Barrel Temperature 180 - 200 °C356 - 392 °FInjection Molding
 180 - 200 °C356 - 392 °FTransition, Extrusion
Front Barrel Temperature 200 - 220 °C392 - 428 °FInjection Molding
 220 - 230 °C428 - 446 °FExtrusion
Nozzle Temperature 220 - 230 °C428 - 446 °FInjection Molding
Die Temperature 195 - 210 °C383 - 410 °FExtrusion
Melt Temperature 180 - 230 °C356 - 446 °FInjection Molding
 180 - 230 °C356 - 446 °FExtrusion
Mold Temperature 25.0 - 40.0 °C77.0 - 104 °FInjection Molding
Injection Pressure 5.00 - 40.0 MPa725 - 5800 psiInjection Molding
Back Pressure 0.500 - 1.00 MPa72.5 - 145 psiInjection Molding
Screw Speed 60 - 100 rpm60 - 100 rpmExtrusion
 100 - 200 rpm100 - 200 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company ESD C 2700-75A Saturated Styrenic Block Copolymer, ESD Protection - Electrically Conductive
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer
Termopol Termoton® K2GA3060A TPE Compound, based on SEBS and Polyolefins
Stellarchem AB860EM TPE Compound
Noble Polymers Regis™ 190108 Thermoplastic Olefin (TPO)

PSTELL002 / 108225

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.