MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay CYCOM® 950-1 Epoxy Prepreg with 38%-G7781
Categories: Polymer; Thermoset; Epoxy

Material Notes: CYCOM® 950-1 modified epoxy resin is a 121°C (250°F) cure system with the performance of a 177°C (350°F) curing epoxy. CYCOM 950-1 prepreg is curable under vacuum-bag-only pressure conditions. CYCOM 950-1 is a controlled flow, net resin content material that offers significant advantages over wet lay-up systems for structural repairs. Advantages include favorable stress-strain characteristics, product quality and consistency, speed of lay-up and vastly improved health and safety characteristics.

Features & Benefits:

  • Aerospace qualified
  • Low outgassing. Approved for space flight
  • Controlled flow material
  • Improved toughness compared with first- and second-generation structural epoxies
  • Dry service temperature of 150°C (300°F) when cured at 135°C (275°F)
  • Mechanical properties of a 177°C (350°F) curing material when cured at 135°C (275°F)
  • Mechanical properties to 104°C (220°F) hot/wet
  • Oven/vacuum bag cure capability as well as autoclave positive pressure cure
  • Efficient for structural repair
  • Conventional drying, lay-up, vacuum bagging and localized low-level heating is all that is required for most applications
  • Shop life of 8 weeks at ambient conditions
  • Suitable for laminate and sandwich panel usage
  • Co-curable with various aerospace qualified adhesive materials
Suggested Applications:
  • Helicopter fuselage and rotor components
  • Wing structures
  • Field repairs and permanent repairs
  • Space flight applications

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Outgassing - Total Mass Loss 0.24 %0.24 %RML
 0.50 - 0.70 %0.50 - 0.70 %TML
Collected Volatile Condensable Material 0.020 - 0.040 %0.020 - 0.040 %
Storage Temperature <= -18.0 °C<= -0.400 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  237 MPa
@Temperature 121 °C
34400 psi
@Temperature 250 °F
90° orientation
 279 MPa
@Temperature 93.0 °C
40500 psi
@Temperature 199 °F
90° orientation
 320 MPa
@Temperature 121 °C
46400 psi
@Temperature 250 °F
0° orientation
 344 MPa
@Temperature 93.0 °C
49900 psi
@Temperature 199 °F
0° orientation
 376 MPa
@Temperature 24.0 °C
54500 psi
@Temperature 75.2 °F
90° orientation
 462 MPa
@Temperature 24.0 °C
67000 psi
@Temperature 75.2 °F
0° orientation
 476 MPa
@Temperature -55.0 °C
69100 psi
@Temperature -67.0 °F
90° orientation
 549 MPa
@Temperature -55.0 °C
79600 psi
@Temperature -67.0 °F
0° orientation
Tensile Modulus  12.5 GPa
@Temperature 121 °C
1810 ksi
@Temperature 250 °F
0° orientation
 14.6 GPa
@Temperature 121 °C
2120 ksi
@Temperature 250 °F
90° orientation
 16.6 GPa
@Temperature 93.0 °C
2410 ksi
@Temperature 199 °F
90° orientation
 20.5 GPa
@Temperature 93.0 °C
2970 ksi
@Temperature 199 °F
0° orientation
 20.6 GPa
@Temperature 24.0 °C
2990 ksi
@Temperature 75.2 °F
90° orientation
 22.6 GPa
@Temperature -55.0 °C
3280 ksi
@Temperature -67.0 °F
90° orientation
 23.0 GPa
@Temperature 24.0 °C
3340 ksi
@Temperature 75.2 °F
0° orientation
 25.8 GPa
@Temperature -55.0 °C
3740 ksi
@Temperature -67.0 °F
0° orientation
Flexural Strength  268 MPa
@Temperature 121 °C
38800 psi
@Temperature 250 °F
0° orientation
 365 MPa
@Temperature 93.0 °C
52900 psi
@Temperature 199 °F
0° orientation
 648 MPa
@Temperature 24.0 °C
94000 psi
@Temperature 75.2 °F
0° orientation
 865.3 MPa
@Temperature -55.0 °C
125500 psi
@Temperature -67.0 °F
0° orientation
Flexural Modulus  16.2 GPa
@Temperature 121 °C
2350 ksi
@Temperature 250 °F
0° orientation
 19.9 GPa
@Temperature 93.0 °C
2890 ksi
@Temperature 199 °F
0° orientation
 20.8 GPa
@Temperature -55.0 °C
3020 ksi
@Temperature -67.0 °F
0° orientation
 22.3 GPa
@Temperature 24.0 °C
3230 ksi
@Temperature 75.2 °F
0° orientation
Compressive Strength  232 MPa
@Temperature 121 °C
33600 psi
@Temperature 250 °F
0° orientation
 233 MPa
@Temperature 121 °C
33800 psi
@Temperature 250 °F
90° orientation
 274 MPa
@Temperature 93.0 °C
39700 psi
@Temperature 199 °F
90° orientation
 352 MPa
@Temperature 93.0 °C
51100 psi
@Temperature 199 °F
0° orientation
 428 MPa
@Temperature 24.0 °C
62100 psi
@Temperature 75.2 °F
90° orientation
 500 MPa
@Temperature 24.0 °C
72500 psi
@Temperature 75.2 °F
0° orientation
 510 MPa
@Temperature -55.0 °C
74000 psi
@Temperature -67.0 °F
90° orientation
 630 MPa
@Temperature -55.0 °C
91400 psi
@Temperature -67.0 °F
0° orientation
Shear Modulus  2.10 GPa
@Temperature 121 °C
305 ksi
@Temperature 250 °F
In Plane
 5.00 GPa
@Temperature 93.0 °C
725 ksi
@Temperature 199 °F
In Plane
 11.9 GPa
@Temperature 24.0 °C
1730 ksi
@Temperature 75.2 °F
In Plane
 16.1 GPa
@Temperature -55.0 °C
2340 ksi
@Temperature -67.0 °F
In Plane
Shear Strength  20.7 MPa
@Temperature 121 °C
3000 psi
@Temperature 250 °F
Interlaminar
 30.3 MPa
@Temperature 93.0 °C
4400 psi
@Temperature 199 °F
Interlaminar
 66.9 MPa
@Temperature -55.0 °C
9700 psi
@Temperature -67.0 °F
Interlaminar
 67.6 MPa
@Temperature 24.0 °C
9800 psi
@Temperature 75.2 °F
Interlaminar
 95.8 MPa
@Temperature 121 °C
13900 psi
@Temperature 250 °F
In Plane
 117 MPa
@Temperature 93.0 °C
17000 psi
@Temperature 199 °F
In Plane
 191 MPa
@Temperature 24.0 °C
27700 psi
@Temperature 75.2 °F
In Plane
 266 MPa
@Temperature -55.0 °C
38600 psi
@Temperature -67.0 °F
In Plane
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 104 °C220 °F
 
Processing PropertiesMetricEnglishComments
Gel Time 13.0 min
@Temperature 135 °C
13.0 min
@Temperature 275 °F
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay CYCOM® 919 Epoxy Prepreg System with Woven E Glass Fiber 7781
Park Aerospace Nelcote® E-722 Epoxy Prepreg, 7781 E-Glass Reinforced
Solvay CYCOM® 381 Epoxy E-glass Prepreg
Solvay CYCOM® 381 Epoxy Prepreg with E-glass Fabric and 300FAW Epoxy
Park Aerospace Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced

PCYTED154_3 / 192664

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.