MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay CYCOM® 381 Epoxy E-glass Prepreg
Categories: Polymer; Thermoset; Epoxy

Material Notes: CYCOM 381 with 120 e-glass fabric and 107FAW epoxy

CYCOM® 381 epoxy prepreg is an epoxy prepreg that offers a 250°F (121°C) curing system with high 180°F (82°C)/wet mechanical properties yet has the excellent fatigue and durability necessary for primary structure applications.

Features & Benefits:

  • Excellent 180°F (82°C)/wet properties
  • Service temperature to 220°F (104°C)
  • Three- to four-fold increases in fatigue life compared to perhaps all conventional 250°F (121°C) curing epoxy prepregs. This increase is the result of a 10 – 15% higher strain endurance limit.
  • Inherent toughness provides good durability and compression after impact performance
  • Low moisture absorption
  • Excellent for vacuum pressure/oven processing
Applications:
  • Primary and secondary structural aircraft parts requiring 180°F (82°C)/wet retention of properties and/or excellent fatigue behavior
  • Components that require good durability and/or low processing temperatures
  • Helicopter rotor blades
  • Rotating or cycled components
  • Co-cured aluminum assemblies/parts
  • Doublers
  • Propellers
  • Composite repair

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  483 MPa
@Temperature 104 °C
70100 psi
@Temperature 219 °F
Warp, dry; SACMA SRM-4
 544 MPa
@Temperature 22.0 °C
78900 psi
@Temperature 71.6 °F
Warp, dry; SACMA SRM-4
Tensile Modulus  25.6 GPa
@Temperature 104 °C
3710 ksi
@Temperature 219 °F
Warp, dry; SACMA SRM-4
 27.4 GPa
@Temperature 22.0 °C
3970 ksi
@Temperature 71.6 °F
Warp, dry; SACMA SRM-4
Flexural Strength  731 MPa
@Temperature 104 °C
106000 psi
@Temperature 219 °F
3-point
 786 MPa
@Temperature 22.0 °C
114000 psi
@Temperature 71.6 °F
3-point
Flexural Modulus  26.0 GPa
@Temperature 22.0 °C
3770 ksi
@Temperature 71.6 °F
3-point; ASTM D790
 28.0 GPa
@Temperature 104 °C
4060 ksi
@Temperature 219 °F
3-point; ASTM D790
Compressive Strength  621 MPa
@Temperature 104 °C
90100 psi
@Temperature 219 °F
Warp, dry; SACMA SRM-1
 696 MPa
@Temperature 22.0 °C
101000 psi
@Temperature 71.6 °F
Warp, dry; SACMA SRM-1
Shear Strength 66.9 MPa9700 psiShort Beam; SACMA SRM-8
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 104 °C219 °F
 
Processing PropertiesMetricEnglishComments
Gel Time 5.00 - 8.00 min
@Temperature 121 °C
5.00 - 8.00 min
@Temperature 250 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay CYCOM® 381 Epoxy Prepreg with E-glass Fabric and 300FAW Epoxy
Solvay CYCOM® 381 Epoxy Prepreg with AS4 Graphite Fabric and 195FAW Epoxy
Solvay CYCOM® 381 Epoxy Prepreg with AS4 Uni-graphite and 145FAW Epoxy
Solvay CYCOM® 381 Epoxy Prepreg with CYCOM 7781 OST E-glass Fabric and 300FAW Epoxy
Park Aerospace Nelcote® E-722 Epoxy Prepreg, 7781 E-Glass Reinforced

PCYTED078 / 180380

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.