MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum Oxyhydroxide, AlO(OH), Boehmite
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: CAS Number: 14457-84-2

Physical Form: Orthorhombic Crystals

Key Words: Aluminum Oxyhydroxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.44 g/cc0.124 lb/in³
a Lattice Constant 2.868 Å2.868 Å
b Lattice Constant 12.23 Å12.23 Å
c Lattice Constant 3.692 Å3.692 Å
Formula Units/Cell (Z) 44
Molecular Weight 59.989 g/mol59.989 g/mol
 
Chemical PropertiesMetricEnglishComments
Molar Volume 19.55 cc/mol19.55 cc/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 3.5 - 43.5 - 4
 
Electrical PropertiesMetricEnglishComments
Magnetic Susceptibility -3.70e-7-3.70e-7
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  0.840 J/g-°C
@Temperature 24.9 °C
0.201 BTU/lb-°F
@Temperature 76.7 °F
Calculated
 1.04 J/g-°C
@Temperature 127 °C
0.249 BTU/lb-°F
@Temperature 260 °F
Calculated
 1.09 J/g-°C
@Temperature 25.0 °C
0.261 BTU/lb-°F
@Temperature 77.0 °F
Crystalline
 1.18 J/g-°C
@Temperature 227 °C
0.282 BTU/lb-°F
@Temperature 440 °F
Calculated
 1.31 J/g-°C
@Temperature 327 °C
0.313 BTU/lb-°F
@Temperature 620 °F
Calculated
Heat of Formation -990.4 kJ/mol-990.4 kJ/molCrystalline
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.6491.649na
 1.6591.659nß
 1.665
@Wavelength 435.8 nm
1.665
@Wavelength 435.8 nm
ng
 
Descriptive Properties
Cleavage(010)
SolubilityInsoluble in H2O; Soluble in Acid and Alkaline Solutions
SynonymBoehmite

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Oxyhydroxide, AlO(OH), Diaspore
Nabaltec APYRAL® AOH 60 AlO(OH) Boehmite
Alumina, alpha Al2O3, 96%
Alpha Calcit Alfrimal 446 Aluminum Hydroxide 99.5%
Albite (Plagioclase Feldspar NaAlSi3O8)

EINOR2023 / 4164

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.