MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aluminum Oxyhydroxide, AlO(OH), Boehmite
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: CAS Number: 14457-84-2

Physical Form: Orthorhombic Crystals

Key Words: Aluminum Oxyhydroxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.44 g/cc
a Lattice Constant 2.868 Å
b Lattice Constant 12.23 Å
c Lattice Constant 3.692 Å
Formula Units/Cell (Z) 4
Molecular Weight 59.989 g/mol
 
Chemical PropertiesOriginal ValueComments
Molar Volume 19.55 cc/mol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 3.5 - 4
 
Electrical PropertiesOriginal ValueComments
Magnetic Susceptibility -3.70e-7
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.840 J/g-°C
@Temperature 24.9 °C
Calculated
 1.04 J/g-°C
@Temperature 127 °C
Calculated
 1.09 J/g-°C
@Temperature 25.0 °C
Crystalline
 1.18 J/g-°C
@Temperature 227 °C
Calculated
 1.31 J/g-°C
@Temperature 327 °C
Calculated
Heat of Formation -990.4 kJ/molCrystalline
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.649na
 1.659nß
 1.665
@Wavelength 435.8 nm
ng
 
Descriptive Properties
Cleavage(010)
SolubilityInsoluble in H2O; Soluble in Acid and Alkaline Solutions
SynonymBoehmite

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum Oxyhydroxide, AlO(OH), Diaspore
Nabaltec APYRAL® AOH 60 AlO(OH) Boehmite
Alumina, alpha Al2O3, 96%
Alpha Calcit Alfrimal 446 Aluminum Hydroxide 99.5%
Albite (Plagioclase Feldspar NaAlSi3O8)

EINOR2023 / 4164

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.