MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum Oxyhydroxide, AlO(OH), Diaspore
Categories: Ceramic; Oxide; Aluminum Oxide

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.44 g/cc0.124 lb/in³
a Lattice Constant 4.396 Å4.396 Å
b Lattice Constant 9.426 Å9.426 Å
c Lattice Constant 2.844 Å2.844 Å
Formula Units/Cell (Z) 44
Molecular Weight 59.989 g/mol59.989 g/mol
 
Chemical PropertiesMetricEnglishComments
Molar Volume 17.76 cc/mol17.76 cc/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 6.5 - 76.5 - 7
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  0.680 J/g-°C
@Temperature 24.9 °C
0.163 BTU/lb-°F
@Temperature 76.7 °F
Calculated
 0.840 J/g-°C
@Temperature 127 °C
0.201 BTU/lb-°F
@Temperature 260 °F
Calculated
 0.890 J/g-°C
@Temperature 25.0 °C
0.213 BTU/lb-°F
@Temperature 77.0 °F
Crystalline
 0.960 J/g-°C
@Temperature 227 °C
0.229 BTU/lb-°F
@Temperature 440 °F
Calculated
 1.06 J/g-°C
@Temperature 327 °C
0.253 BTU/lb-°F
@Temperature 620 °F
Calculated
Heat of Formation -999.8 kJ/mol-999.8 kJ/molCrystalline
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.7021.702na
 1.7221.722nß
 1.75
@Wavelength 435.8 nm
1.75
@Wavelength 435.8 nm
ng
 
Descriptive Properties
BrittlenessBrittle
Cleavage(010)Perfect
Crystal StructureOrthorhombic
LusterBrilliant Pearl
SolubilityInsoluble in H2O

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Oxyhydroxide, AlO(OH), Boehmite
AISI Type M3 Class 1 Molybdenum High Speed Tool Steel (UNS T11313)
Nabaltec APYRAL® AOH 60 AlO(OH) Boehmite
AISI Type H13 Hot Work Tool Steel
AISI 8620 Steel, quenched from 900°C (1650°F), tempered at 425°C (800°F), Low temp impact properties

EINOR2023b / 135564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.