Optimum for Black and Darker Colors below 50L value. Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Ductile/Brittle transition as measured by Instrumented Impact is 5 deg.C Physical properties based on Geon HTX Ultra LA425 Natural 0000 Geon Performance Solutions was created from PolyOne in 2019. |