MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions HTX Ultra LA426 Tan 3725 Polyvinyl Chloride Alloy (PVC Alloy)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.

Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties of Geon HTX Ultra LA426 Tan 3725

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.26 g/cc1.26 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 767615 sec; ASTM D2240
Tensile Strength, Yield 38.4 MPa5570 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.04 GPa296 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 66.9 MPa9700 psiASTM D790
Flexural Modulus 2.09 GPa303 ksiASTM D790
Izod Impact, Notched 6.90 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
12.9 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
Dart Drop Total Energy  59.6 J/cm
@Temperature 23.0 °C
0.112 ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
 178 J/cm
@Temperature 23.0 °C
0.333 ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C44.4 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi)  91.1 °C
@Thickness 3.18 mm
196 °F
@Thickness 0.125 in
Unannealed; ASTM D648
 91.1 °C
@Thickness 3.18 mm
196 °F
@Thickness 0.125 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)  82.2 °C
@Thickness 3.18 mm
180 °F
@Thickness 0.125 in
Unannealed; ASTM D648
 86.1 °C
@Thickness 3.18 mm
187 °F
@Thickness 0.125 in
Annealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 174 - 193 °C345 - 379 °F
 
Descriptive Properties
Ease of SizingAcceptable
FeaturesHigh Impact Resistance
 High Stiffness
FormsPellets
Generic MaterialPVC Alloy
Generic NamePolyvinyl Chloride Alloy (PVC Alloy)
Processing MethodExtrusion
PVC Cell Classification15225ASTM D1784
 4-41421-64-0000ASTM D4216
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesOutdoor Applications
 Profiles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions HTX Ultra LA426 Black 2880 Polyvinyl Chloride Alloy (PVC Alloy)
Geon® Performance Solutions HTX L1502 Polyvinyl Chloride Alloy (PVC Alloy)
Geon® Performance Solutions HTX Ultra LA426 Gray 2382 Polyvinyl Chloride Alloy (PVC Alloy)
Geon® Performance Solutions HTX Ultra LA426 PVC Alloy
INEOS Styrolution Luran® S 776SE ASA

PH0POL0898 / 145467

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.